Unsung Heroes of Energy Research AITranslate
Publisher: ACS
Abstract AITranslate
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.8b00792
Chinese Library Classification Number:
Citation Information:
quote
| GB/T 7714-2015 | [1] Prashant V. Kamat. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.8b00792. |
| MLA | [1] Prashant V. Kamat. ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.8b00792. |
| APA | [1] Prashant V. Kamat. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.8b00792 |
| IEEE | [1] Prashant V. Kamat, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.8b00792. |