Highly Conductive Polydopamine Coatings by Direct Electrochemical Synthesis on Au AITranslate

Inha University; University of Delaware; Inha University; Inha University; Inha University; University of Delaware; Inha University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Polydopamine (PDA) is a promising melanin-like material with unique properties such as hybrid electronic–ionic conductivity, UV–vis light absorption, wet adhesion, biocompatibility, anti-inflammation, and metal ion chelation. Despite its versatility, PDA has limited utilization in bioelectronics due to its low electrochemical conductivity. Here, we present an electrochemical synthesis for highly conductive PDA composites directly coated on Au electrodes. PDA was deposited by the confined oxidizing effect of dissolved Au3+ on the electrode, which produced unprecedentedly conductive PDAs. The impedance of the Au electrode decreases by 2 orders of magnitude at 1 kHz, and both the ionic charge storage capacity and the safe charge injection limit increase by 1 order of magnitude, respectively. Unlike conventional conducting polymers, the PDA composite provides durable electrochemical performances after 1000 cyclic voltammetry (CV) cycles between −0.6 and 0.8 V. Furthermore, the PDA/Au showed remarkable structural modulation from fluffy to dense PDA as well as the efficient charge-transfer capability for both cationic and anionic carriers compared to the Au electrode. This unique PDA composite can be used as a conductive bioorganic material to develop edible/implantable/biodegradable electrodes, biosensors, and neuromorphic electrochemical devices for future bioelectronic applications.

KeyWords AITranslate

dopamine polydopamine electrochemical deposition conductive biomaterials conductive polydopamine
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c00317

Chinese Library Classification Number:

Citation Information:

Polydopamine (PDA) is a promising melanin-like material with unique properties such as hybrid electronic–ionic conductivity, UV–vis light absorption, wet adhesion, biocompatibility, anti-inflammation, and metal ion chelation. Despite its versatility, PDA has limited utilization in bioelectronics due to its low electrochemical conductivity. Here, we present an electrochemical synthesis for highly conductive PDA composites directly coated on Au electrodes. PDA was deposited by the confined oxidizing effect of dissolved Au3+ on the electrode, which produced unprecedentedly conductive PDAs. The impedance of the Au electrode decreases by 2 orders of magnitude at 1 kHz, and both the ionic charge storage capacity and the safe charge injection limit increase by 1 order of magnitude, respectively. Unlike conventional conducting polymers, the PDA composite provides durable electrochemical performances after 1000 cyclic voltammetry (CV) cycles between −0.6 and 0.8 V. Furthermore, the PDA/Au showed remarkable structural modulation from fluffy to dense PDA as well as the efficient charge-transfer capability for both cationic and anionic carriers compared to the Au electrode. This unique PDA composite can be used as a conductive bioorganic material to develop edible/implantable/biodegradable electrodes, biosensors, and neuromorphic electrochemical devices for future bioelectronic applications.

quote

GB/T 7714-2015 [1] Taesik Eom, Junghyun Lee, Seunghyeon Lee, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c00317.
MLA [1] Taesik Eom, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c00317.
APA [1] Taesik Eom, Junghyun Lee, Seunghyeon Lee, Busra Ozlu, Sunwoo Kim, David C. Martin, & Bong Sup Shim. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c00317
IEEE [1] Taesik Eom, Junghyun Lee, Seunghyeon Lee, Busra Ozlu, Sunwoo Kim, David C. Martin, and Bong Sup Shim, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c00317. keywords: {dopamine;polydopamine;electrochemical deposition;conductive biomaterials;conductive polydopamine}