Abstract AITranslate
Cesium lead halide perovskite nanocrystals (PNCs) have enjoyed enormous attention in optoelectronics and photovoltaics. However, instability under polar conditions and limited energy/charge transport due to long-chain capping ligands restrict their large-scale applications. We have engineered a short-chain multidentate bolaamphiphilic ligand (NKE-3), which provides synergistic passivation of the perovskite surface by one multidentate ionic terminal and localizes water molecules by another multidentate ionic terminal, leading to a water-suspended colloidal solution of PNCs. NKE-3 allows efficient long-range dipole-based fluorescence resonance energy transfer (FRET) from perovskites to Rhodamine B isothiocyanate (RITC) in water, with FRET efficiencies ranging from 96% to 98%. We calculated the FRET rate using the acceptor’s rise-time component, as it ensures no contamination from FRET-inactive donors. Moreover, we tuned the emission maxima of PNCs through halide exchange to optimize FRET efficiency. Such energy funneling to a suitable molecular photocatalyst is imperative for PNCs’ potential applications.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.3c00197
Chinese Library Classification Number:
Citation Information:
Cesium lead halide perovskite nanocrystals (PNCs) have enjoyed enormous attention in optoelectronics and photovoltaics. However, instability under polar conditions and limited energy/charge transport due to long-chain capping ligands restrict their large-scale applications. We have engineered a short-chain multidentate bolaamphiphilic ligand (NKE-3), which provides synergistic passivation of the perovskite surface by one multidentate ionic terminal and localizes water molecules by another multidentate ionic terminal, leading to a water-suspended colloidal solution of PNCs. NKE-3 allows efficient long-range dipole-based fluorescence resonance energy transfer (FRET) from perovskites to Rhodamine B isothiocyanate (RITC) in water, with FRET efficiencies ranging from 96% to 98%. We calculated the FRET rate using the acceptor’s rise-time component, as it ensures no contamination from FRET-inactive donors. Moreover, we tuned the emission maxima of PNCs through halide exchange to optimize FRET efficiency. Such energy funneling to a suitable molecular photocatalyst is imperative for PNCs’ potential applications.
quote
| GB/T 7714-2015 | [1] Pooja Aggarwal, Anubhab Halder, Neelakshi, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c00197. |
| MLA | [1] Pooja Aggarwal, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c00197. |
| APA | [1] Pooja Aggarwal, Anubhab Halder, Neelakshi, Ramesh Ramapanicker, & Vishal Govind Rao. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c00197 |
| IEEE | [1] Pooja Aggarwal, Anubhab Halder, Neelakshi, Ramesh Ramapanicker, and Vishal Govind Rao, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c00197. |