Water/Salt Transport Properties of Polyamide Reverse Osmosis Membranes Using Quartz Crystal Microbalance AITranslate

Tiangong University; Tiangong University; Henan Normal University; Tiangong University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Thin-film composite (TFC) reverse osmosis (RO) membranes prepared by interfacial polymerization of M-phenylene diamine (MPD) and trimesoyl chloride (TMC) are the most widely used membranes in the current desalination market. However, how to accurately and quantitatively describe the permeation process that quantifies the water/salt partition coefficient (K) and the diffusivity coefficient (D) of the polyamide matrix in the polyamide active layer remains a challenge. Herein, the water and salt transport properties of polyamide (PA) TFC membranes are systematically investigated for the first time based on the quartz crystal microbalance with dissipation (QCM-D), and the relationships between structure and transport properties are investigated. The change of water/salt participation (Kw and Ks) with the TMC concentration is much more sensitive than that with the MPD concentration increase. The Kw slightly changes with increasing monomer concentrations, while the Ks increases first and then remains almost unchanged with an increase in the TMC concentration. There is a significant reduction of the Dw and Ds of the polyamide matrix by enhancing the cross-linking degree as the TMC concentration increased from 0.05 to 0.125%. Enhancing the cross-linking degree of the polyamide matrix by adjusting the monomer concentration is beneficial to improve water/salt diffusivity selectivity. The evolving trend of permeability is consistent with the diffusivity, indicating that the permeability of the polyamide TFC membrane is mainly determined by the diffusivity of the polyamide matrix. In conclusion, varying the TMC concentration is more likely to change the physicochemical properties of the polyamide active layers, including water/salt transport properties.

KeyWords AITranslate

polyamide reverse osmosis water/salt transport properties Qsense quartz crystal microbalance with dissipation (QCMD) Show More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c01194

Chinese Library Classification Number:

Citation Information:

Thin-film composite (TFC) reverse osmosis (RO) membranes prepared by interfacial polymerization of M-phenylene diamine (MPD) and trimesoyl chloride (TMC) are the most widely used membranes in the current desalination market. However, how to accurately and quantitatively describe the permeation process that quantifies the water/salt partition coefficient (K) and the diffusivity coefficient (D) of the polyamide matrix in the polyamide active layer remains a challenge. Herein, the water and salt transport properties of polyamide (PA) TFC membranes are systematically investigated for the first time based on the quartz crystal microbalance with dissipation (QCM-D), and the relationships between structure and transport properties are investigated. The change of water/salt participation (Kw and Ks) with the TMC concentration is much more sensitive than that with the MPD concentration increase. The Kw slightly changes with increasing monomer concentrations, while the Ks increases first and then remains almost unchanged with an increase in the TMC concentration. There is a significant reduction of the Dw and Ds of the polyamide matrix by enhancing the cross-linking degree as the TMC concentration increased from 0.05 to 0.125%. Enhancing the cross-linking degree of the polyamide matrix by adjusting the monomer concentration is beneficial to improve water/salt diffusivity selectivity. The evolving trend of permeability is consistent with the diffusivity, indicating that the permeability of the polyamide TFC membrane is mainly determined by the diffusivity of the polyamide matrix. In conclusion, varying the TMC concentration is more likely to change the physicochemical properties of the polyamide active layers, including water/salt transport properties.

quote

GB/T 7714-2015 [1] Mingguang Hu, Chenchen Zhang, Meng You, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c01194.
MLA [1] Mingguang Hu, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c01194.
APA [1] Mingguang Hu, Chenchen Zhang, Meng You, & Jianqiang Meng. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c01194
IEEE [1] Mingguang Hu, Chenchen Zhang, Meng You, and Jianqiang Meng, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c01194. keywords: {polyamide;reverse osmosis;water/salt transport properties;Qsense quartz crystal microbalance with dissipation (QCMD);Show More}