Self-Healable and Injectable Nanocomposite Hydrogel Loading Iron-Doped Carbon Dots for Synergistic Antibacterial Peptide-Photothermal-Photodynamic Antibacterial Therapy AITranslate

The Fifth Affiliated Hospital of Zhengzhou University; Tongji University; Tongji University;Tenth People’s Hospital Affiliated to Tongji University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The abuse of antibiotics greatly increases the risk of bacterial resistance. Therefore, it is crucial to develop an efficient nonantibiotic antibacterial treatment strategy. As a result, a self-healable and injectable nanocomposite hydrogel with synergistic antibacterial peptide-photothermal (PTT)-photodynamic (PDT) antibacterial activities was designed and fabricated. The nanocomposite hydrogel was prepared through the facile mixing of hydroxypropyl chitosan-graft-ε-poly(l-lysine) (HPCS-g-EPL), oxidized dextran (OD), and iron-doped carbon dots (Fe-CDs) with the formation of Schiff base bond between HPCS-g-EPL and OD. With the hydrolysis of an amide bond in the hydrogel, EPL grafted onto HPCS will be released continuously. Under near-infrared irradiation for 10 min, Fe-CDs can act as photothermal therapeutic agents to generate heat (approximately 50 °C) and photodynamic therapeutic agents to rapidly catalyze the decomposition of hydrogen peroxide to produce hydroxyl radicals. After the treatment of synergistic antibacterial treatment, the antibacterial rate against Escherichia coli and Staphylococcus aureus can reach more than 99%. Therefore, the antibacterial peptide (EPL)-PTT-PDT synergistic antibacterial therapy strategy without antibiotics has broad prospects in the field of bacterial infection treatment.

KeyWords AITranslate

selfhealable and injectable nanocomposite hydrogel irondoped carbon dots εpoly(llysine) synergistic antibacterial
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c02024

Chinese Library Classification Number:

Citation Information:

The abuse of antibiotics greatly increases the risk of bacterial resistance. Therefore, it is crucial to develop an efficient nonantibiotic antibacterial treatment strategy. As a result, a self-healable and injectable nanocomposite hydrogel with synergistic antibacterial peptide-photothermal (PTT)-photodynamic (PDT) antibacterial activities was designed and fabricated. The nanocomposite hydrogel was prepared through the facile mixing of hydroxypropyl chitosan-graft-ε-poly(l-lysine) (HPCS-g-EPL), oxidized dextran (OD), and iron-doped carbon dots (Fe-CDs) with the formation of Schiff base bond between HPCS-g-EPL and OD. With the hydrolysis of an amide bond in the hydrogel, EPL grafted onto HPCS will be released continuously. Under near-infrared irradiation for 10 min, Fe-CDs can act as photothermal therapeutic agents to generate heat (approximately 50 °C) and photodynamic therapeutic agents to rapidly catalyze the decomposition of hydrogen peroxide to produce hydroxyl radicals. After the treatment of synergistic antibacterial treatment, the antibacterial rate against Escherichia coli and Staphylococcus aureus can reach more than 99%. Therefore, the antibacterial peptide (EPL)-PTT-PDT synergistic antibacterial therapy strategy without antibiotics has broad prospects in the field of bacterial infection treatment.

quote

GB/T 7714-2015 [1] Anqin Dong, Wenrui Xiao, Weizhong Yuan, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c02024.
MLA [1] Anqin Dong, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c02024.
APA [1] Anqin Dong, Wenrui Xiao, Weizhong Yuan, & Keqiang Zuo. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c02024