daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Enhanced Durability of Automotive Fuel Cells via Selectivity Implementation by Hydrogen Spillover on the Electrocatalyst Surface AITranslate

Pohang University of Science and Technology; Pohang University of Science and Technology; Pohang University of Science and Technology; Pohang University of Science and Technology; Korea Advanced Institute of Science and Technology; Sogang University; Korea Advanced Institute of Science and Technology; Korea Advanced Institute of Science and Technology; Sogang University; Korea Advanced Institute of Science and Technology; Pohang University of Science and Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Startup and shutdown (SU/SD) events in automotive polymer electrolyte membrane fuel cells cause an unintended oxygen reduction reaction (ORR) due to the mixing of air in the anode, leading to instantaneous potential jumps and subsequent carbon corrosion in the cathode. Here, a selective electrocatalysis method for the hydrogen oxidation reaction (HOR) is presented as a promising approach for inhibiting the ORR and preventing cathodic corrosion during SU/SD events. Platinum (Pt) supported on titanium dioxide (TiO2) demonstrated HOR-selective electrocatalysis, made possible by extreme variation in conductivity according to the hydrogen concentration in the atmosphere. Under hydrogen-rich conditions, hydrogen spillover occurred and led to the formation of a conduction pathway on the Pt/TiO2 surface, promoting the HOR. Under oxygen-rich conditions, the conductivity of the TiO2 surface caused it to return to its original insulating nature, inhibiting the ORR. In an SU/SD simulation protocol test, the HOR-selective Pt/TiO2 demonstrated three-times-higher durability in a membrane electrode assembly in comparison with a commercial Pt/C catalyst.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.2c02656

Chinese Library Classification Number:

Citation Information:

Startup and shutdown (SU/SD) events in automotive polymer electrolyte membrane fuel cells cause an unintended oxygen reduction reaction (ORR) due to the mixing of air in the anode, leading to instantaneous potential jumps and subsequent carbon corrosion in the cathode. Here, a selective electrocatalysis method for the hydrogen oxidation reaction (HOR) is presented as a promising approach for inhibiting the ORR and preventing cathodic corrosion during SU/SD events. Platinum (Pt) supported on titanium dioxide (TiO2) demonstrated HOR-selective electrocatalysis, made possible by extreme variation in conductivity according to the hydrogen concentration in the atmosphere. Under hydrogen-rich conditions, hydrogen spillover occurred and led to the formation of a conduction pathway on the Pt/TiO2 surface, promoting the HOR. Under oxygen-rich conditions, the conductivity of the TiO2 surface caused it to return to its original insulating nature, inhibiting the ORR. In an SU/SD simulation protocol test, the HOR-selective Pt/TiO2 demonstrated three-times-higher durability in a membrane electrode assembly in comparison with a commercial Pt/C catalyst.

quote

GB/T 7714-2015 [1] SangHoon You, SangMun Jung, KyuSu Kim, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.2c02656.
MLA [1] SangHoon You, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.2c02656.
APA [1] SangHoon You, SangMun Jung, KyuSu Kim, Jinhyeon Lee, Jinkyu Park, Ho Yeon Jang, Sangyong Shin, Hyunjoo Lee, Seoin Back, Jinwoo Lee, & YongTae Kim. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.2c02656
IEEE [1] SangHoon You, SangMun Jung, KyuSu Kim, Jinhyeon Lee, Jinkyu Park, Ho Yeon Jang, Sangyong Shin, Hyunjoo Lee, Seoin Back, Jinwoo Lee, and YongTae Kim, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.2c02656.