Spatial Management of CO Diffusion on Tandem Electrode Promotes NH2 Intermediate Formation for Efficient Urea Electrosynthesis AITranslate

Hefei University of Technology; Hefei University of Technology; Hefei University of Technology; University of Cincinnati; Hefei University of Technology; Hefei University of Technology; Hefei University of Technology; University of Cincinnati; Hefei University of Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Electrocatalytic urea synthesis is a promising alternative to the energy-intensive conventional industrial process. However, it lacks highly active and selective catalyst systems. Herein, we report a Cu/ZnO stacked tandem gas-diffusion electrode (GDE) for selective urea synthesis from electrocatalytic CO2 and nitrate reduction reactions. The ZnO catalyst layer (CL) segment at the inlet provides a high CO concentration to the downstream Cu CL segment, promoting the conversion of NO3– to *NH2. The CO-mediated NH2 formation accelerates the C–N coupling rate for urea synthesis. As a result, the stacked GDE with an optimal ZnO/Cu CL area ratio achieves a high Faradaic efficiency of 37.4% and a high yield of 3.2 μmol h–1 cm–2 for urea at −0.3 V vs RHE under ambient conditions. This work expands the application of tandem electrodes and realizes the cascade C–N coupling reaction.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.3c00824

Chinese Library Classification Number:

Citation Information:

Electrocatalytic urea synthesis is a promising alternative to the energy-intensive conventional industrial process. However, it lacks highly active and selective catalyst systems. Herein, we report a Cu/ZnO stacked tandem gas-diffusion electrode (GDE) for selective urea synthesis from electrocatalytic CO2 and nitrate reduction reactions. The ZnO catalyst layer (CL) segment at the inlet provides a high CO concentration to the downstream Cu CL segment, promoting the conversion of NO3– to *NH2. The CO-mediated NH2 formation accelerates the C–N coupling rate for urea synthesis. As a result, the stacked GDE with an optimal ZnO/Cu CL area ratio achieves a high Faradaic efficiency of 37.4% and a high yield of 3.2 μmol h–1 cm–2 for urea at −0.3 V vs RHE under ambient conditions. This work expands the application of tandem electrodes and realizes the cascade C–N coupling reaction.

quote

GB/T 7714-2015 [1] Yan Wang, Shuai Xia, Jianfang Zhang, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c00824.
MLA [1] Yan Wang, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c00824.
APA [1] Yan Wang, Shuai Xia, Jianfang Zhang, Zhengyuan Li, Rui Cai, Cuiping Yu, Yong Zhang, Jingjie Wu, & Yucheng Wu. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c00824
IEEE [1] Yan Wang, Shuai Xia, Jianfang Zhang, Zhengyuan Li, Rui Cai, Cuiping Yu, Yong Zhang, Jingjie Wu, and Yucheng Wu, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c00824.