Injectable hydrogels have gained popularity as an attractive solution for wound dressing therapies due to their ability to conform to irregular wound sites and in situ polymerization. However, the harmful effects of ultraviolet (UV) exposure limit the applicability of photocuring methods, while thermal curing is limited by its high-temperature requirement and nonselective curing. To address these limitations, we present a method of curing hydrogels in situ by incorporating gold nanorods (AuNRs) as microheaters to initiate and regulate local thermal polymerization of the hydrogel upon exposure to near-infrared (NIR) light. In the present method, the well-dispersed AuNRs in the hydrogel presolution enable millions of microheaters to heat up the solution, resulting in a faster kinetic rate and higher polymerization conversion compared to the traditional thermal curing method. Moreover, the NIR light-initiated curing process leads to a more uniform microstructure and improved mechanical performance of hydrogels. This in situ, fast, and selective curing method presents a superior alternative to traditional curing methods and is an ideal choice for wound dressing therapies and other biomedical applications.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.3c00640
Chinese Library Classification Number:
Citation Information:
Injectable hydrogels have gained popularity as an attractive solution for wound dressing therapies due to their ability to conform to irregular wound sites and in situ polymerization. However, the harmful effects of ultraviolet (UV) exposure limit the applicability of photocuring methods, while thermal curing is limited by its high-temperature requirement and nonselective curing. To address these limitations, we present a method of curing hydrogels in situ by incorporating gold nanorods (AuNRs) as microheaters to initiate and regulate local thermal polymerization of the hydrogel upon exposure to near-infrared (NIR) light. In the present method, the well-dispersed AuNRs in the hydrogel presolution enable millions of microheaters to heat up the solution, resulting in a faster kinetic rate and higher polymerization conversion compared to the traditional thermal curing method. Moreover, the NIR light-initiated curing process leads to a more uniform microstructure and improved mechanical performance of hydrogels. This in situ, fast, and selective curing method presents a superior alternative to traditional curing methods and is an ideal choice for wound dressing therapies and other biomedical applications.
quote
| GB/T 7714-2015 | [1] Sirawit Pruksawan, Heng Li Chee, Zizhen Wang, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c00640. |
| MLA | [1] Sirawit Pruksawan, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c00640. |
| APA | [1] Sirawit Pruksawan, Heng Li Chee, Zizhen Wang, Yock Leng Lee, Vinod Kumar S/O Sivaraja, Sian Yang Ow, Jun Li, & FuKe Wang. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c00640 |
| IEEE | [1] Sirawit Pruksawan, Heng Li Chee, Zizhen Wang, Yock Leng Lee, Vinod Kumar S/O Sivaraja, Sian Yang Ow, Jun Li, and FuKe Wang, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c00640. keywords: {gold nanorods;NIR light curing;injectable hydrogel;curing kinetics;wound dressing;microheater} |