A 2.6 V Flexible Supercapacitor Based on Al-MnO2-Na2SO4//AC-KOH with High Specific Energy AITranslate
Abstract AITranslate
In this work, we have synthesized Al-doped MnO2 nanoparticles (Al-MnO2) by rapid coprecipitation followed by hydrothermal and heat treatment. Al-MnO2 shows a specific capacitance of 301.8 F g–1 at 1 A g–1 in a sample of 14% Al-MnO2-260 °C. The specific capacitance still remains at 206 F g–1 at 20 A g–1. It also shows a good cycling stability with no capacitance degradation after 5000 cycles. More importantly, a new type of supercapacitor, Al-MnO2|PVA-Na2SO4//PVA-KOH|AC, has been designed using a Na2SO4-poly(vinyl alcohol)//cation exchange membrane//KOH-poly(vinyl alcohol)-based decoupled electrolyte. This device exhibits a specific capacitance of 68.9 F g–1 at 1 A g–1, corresponding to 64.7 Wh kg–1 at 1300 W kg–1. It also delivers a good capacitance retention of ∼84% after 5000 cycles. The cell voltage is up to 2.6 V, which could light up a green light-emitting diode. The PVA-based decoupled gel electrolyte offers good processability to assemble flexible and foldable devices, which is important for mass production in manufacturing. These results clearly indicate that such high-voltage flexible supercapacitors with high specific energy are very promising in future wearable electronics.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.3c00439
Chinese Library Classification Number:
Citation Information:
In this work, we have synthesized Al-doped MnO2 nanoparticles (Al-MnO2) by rapid coprecipitation followed by hydrothermal and heat treatment. Al-MnO2 shows a specific capacitance of 301.8 F g–1 at 1 A g–1 in a sample of 14% Al-MnO2-260 °C. The specific capacitance still remains at 206 F g–1 at 20 A g–1. It also shows a good cycling stability with no capacitance degradation after 5000 cycles. More importantly, a new type of supercapacitor, Al-MnO2|PVA-Na2SO4//PVA-KOH|AC, has been designed using a Na2SO4-poly(vinyl alcohol)//cation exchange membrane//KOH-poly(vinyl alcohol)-based decoupled electrolyte. This device exhibits a specific capacitance of 68.9 F g–1 at 1 A g–1, corresponding to 64.7 Wh kg–1 at 1300 W kg–1. It also delivers a good capacitance retention of ∼84% after 5000 cycles. The cell voltage is up to 2.6 V, which could light up a green light-emitting diode. The PVA-based decoupled gel electrolyte offers good processability to assemble flexible and foldable devices, which is important for mass production in manufacturing. These results clearly indicate that such high-voltage flexible supercapacitors with high specific energy are very promising in future wearable electronics.
quote
| GB/T 7714-2015 | [1] Jian Yan, Chao Liu, Jiaojiao Yang, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c00439. |
| MLA | [1] Jian Yan, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c00439. |
| APA | [1] Jian Yan, Chao Liu, Jiaojiao Yang, Zhen Wang, Wenxuan Yao, Lulu Huang, Jiewu Cui, Jiaqin Liu, Xiaoye Hu, & Yucheng Wu. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c00439 |
| IEEE | [1] Jian Yan, Chao Liu, Jiaojiao Yang, Zhen Wang, Wenxuan Yao, Lulu Huang, Jiewu Cui, Jiaqin Liu, Xiaoye Hu, and Yucheng Wu, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c00439. |