Controlled Surface Radical Graft Polymerization of N-Halamine Monomers on Polyester Fabrics and Potential Application in Bioprotective Medical Scrubs AITranslate

University of California; University of California; University of California; Shanghai Jiaotong University; University of Shanghai for Science and Technology; University of California
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Embedding medical scrubs with robust biocidal functions could potentially reduce pathogen cross-contamination and healthcare-associated infections. Here, a halamine precursor monomer, 1-acryloyl-2,2,5,5-tetramethylimidazolidin-4-one (ACTMIO), was covalently grafted to a poly(ethylene terephthalate) (PET) fabric, which is a common textile material used in medical scrubs, via a controlled free radical graft polymerization reaction using a “pad-dry-cure” finishing process. Based on a computational model and Hansen solubility theory, an ideal free radical reaction system was designed and implemented. The obtained ACTMIO-grafted (H-PET-g-ACTMIO) fabrics exhibited high grafting ratios of the monomers, desired properties of improved hydrophilicity, large active chlorine capacity, promising chlorine rechargeability, and desirable washing durability due to the robust covalent bonds between halamine moieties and PET fabrics. The chlorinated H-PET-g-ACTMIO fabric demonstrated powerful and regenerable biocidal performance against pathogenic bacteria, revealing the great application potential as a bioprotective medical textile. In addition, the successful application of Hansen solubility theory in surface modification of chemically inert polyester fibers provides a good example of controlling free radical polymerization reactions on textile materials.

KeyWords AITranslate

controlled surface modification polyester fabric halamine Hansen solubility parameters bioprotective medical scrub
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c01223

Chinese Library Classification Number:

Citation Information:

Embedding medical scrubs with robust biocidal functions could potentially reduce pathogen cross-contamination and healthcare-associated infections. Here, a halamine precursor monomer, 1-acryloyl-2,2,5,5-tetramethylimidazolidin-4-one (ACTMIO), was covalently grafted to a poly(ethylene terephthalate) (PET) fabric, which is a common textile material used in medical scrubs, via a controlled free radical graft polymerization reaction using a “pad-dry-cure” finishing process. Based on a computational model and Hansen solubility theory, an ideal free radical reaction system was designed and implemented. The obtained ACTMIO-grafted (H-PET-g-ACTMIO) fabrics exhibited high grafting ratios of the monomers, desired properties of improved hydrophilicity, large active chlorine capacity, promising chlorine rechargeability, and desirable washing durability due to the robust covalent bonds between halamine moieties and PET fabrics. The chlorinated H-PET-g-ACTMIO fabric demonstrated powerful and regenerable biocidal performance against pathogenic bacteria, revealing the great application potential as a bioprotective medical textile. In addition, the successful application of Hansen solubility theory in surface modification of chemically inert polyester fibers provides a good example of controlling free radical polymerization reactions on textile materials.

quote

GB/T 7714-2015 [1] Yue Ma, Cheng Huang, Zheng Zhang, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c01223.
MLA [1] Yue Ma, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c01223.
APA [1] Yue Ma, Cheng Huang, Zheng Zhang, Linlin Xiao, Qingli Dong, & Gang Sun. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c01223
IEEE [1] Yue Ma, Cheng Huang, Zheng Zhang, Linlin Xiao, Qingli Dong, and Gang Sun, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c01223. keywords: {controlled surface modification;polyester fabric;halamine;Hansen solubility parameters;bioprotective medical scrub}