Design Principle of a Water-Dispersed Photocatalytic Perovskite through Ligand Deconstruction AITranslate
Abstract AITranslate
Strategically designed surface modifiers that produce stable perovskite nanocrystals (NCs) and allow efficient charge extraction in polar solvents are critical for perovskite photocatalysis. We designed a multifunctional bolaamphiphilic ligand (NKE-12) with multidentate ionic groups at both ends, which significantly increases the colloidal stability of CsPbBr3 NCs in an aqueous medium without affecting their structural integrity and catalytic attributes. Ligand deconstruction via K and E fragmented ligands revealed synergistic actions of the cationic and anionic functionalities in surface passivation, phase separation, and water localization away from the surface of NKE-12-modified CsPbBr3 NCs. Multidimensional nuclear magnetic resonance experiments and contact angle measurements further suggested surface interactions and improved hydrophilicity via ionic terminal groups that account for water stability. Photogenerated hole-transfer dynamics of CsPbBr3/NKE-12 NCs to a probe molecule 6,7-dihydroxycoumarin was studied using transient absorption spectroscopy. Overall, this study paves the way for ligand design principles for surface engineering to develop water-stable perovskite photocatalysts.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.3c00532
Chinese Library Classification Number:
Citation Information:
Strategically designed surface modifiers that produce stable perovskite nanocrystals (NCs) and allow efficient charge extraction in polar solvents are critical for perovskite photocatalysis. We designed a multifunctional bolaamphiphilic ligand (NKE-12) with multidentate ionic groups at both ends, which significantly increases the colloidal stability of CsPbBr3 NCs in an aqueous medium without affecting their structural integrity and catalytic attributes. Ligand deconstruction via K and E fragmented ligands revealed synergistic actions of the cationic and anionic functionalities in surface passivation, phase separation, and water localization away from the surface of NKE-12-modified CsPbBr3 NCs. Multidimensional nuclear magnetic resonance experiments and contact angle measurements further suggested surface interactions and improved hydrophilicity via ionic terminal groups that account for water stability. Photogenerated hole-transfer dynamics of CsPbBr3/NKE-12 NCs to a probe molecule 6,7-dihydroxycoumarin was studied using transient absorption spectroscopy. Overall, this study paves the way for ligand design principles for surface engineering to develop water-stable perovskite photocatalysts.
quote
| GB/T 7714-2015 | [1] Monika Ahlawat, Neelakshi, Ramesh Ramapanicker, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c00532. |
| MLA | [1] Monika Ahlawat, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c00532. |
| APA | [1] Monika Ahlawat, Neelakshi, Ramesh Ramapanicker, & Vishal Govind Rao. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c00532 |
| IEEE | [1] Monika Ahlawat, Neelakshi, Ramesh Ramapanicker, and Vishal Govind Rao, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c00532. |