Membrane-Induced Vanadium Crossover-Blocking Polybenzimidazole Copolymer with Exceptional Proton Selectivity AITranslate

National Renewable Energy Laboratory; National Renewable Energy Laboratory; University of Tennessee; University of Tennessee; University of Tennessee; National Renewable Energy Laboratory; National Renewable Energy Laboratory
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Broad deployment of redox flow batteries is hindered, in part, due to the lack of highly selective ion-exchange membranes with high proton conductivity. We report a post-functionalization strategy for polybenzimidazole copolymer (PBI-co) membranes by a reacting mixture of concentrated sulfuric and phosphoric acids that led to improved membrane selectivity while retaining high proton conductivity. Fourier-transform infrared spectroscopy confirmed successful sulfonation and protonation of benzimidazole functionalities. PBI-co exhibits a very high room-temperature proton conductivity of 0.138 S cm–1, as measured by electrochemical impedance spectroscopy. PBI-co also demonstrates electromigration crossover mitigation under applied current densities up to 500 mA cm–2, and voltage pulses up to 1.4 V, while also inhibiting diffusion-driven vanadium crossover for over 20 days. Single-cell vanadium flow battery testing on post-functionalized PBI-co further confirms state-of-the-art battery performance with an ∼99.5% Coulombic efficiency at 100 mA cm–2 and an area-specific resistance of ∼20 mΩ cm2 lower than Nafion-212 membrane.

KeyWords AITranslate

membrane polybenzimidazole copolymer proton transport batteries vanadium crossover
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c01318

Chinese Library Classification Number:

Citation Information:

Broad deployment of redox flow batteries is hindered, in part, due to the lack of highly selective ion-exchange membranes with high proton conductivity. We report a post-functionalization strategy for polybenzimidazole copolymer (PBI-co) membranes by a reacting mixture of concentrated sulfuric and phosphoric acids that led to improved membrane selectivity while retaining high proton conductivity. Fourier-transform infrared spectroscopy confirmed successful sulfonation and protonation of benzimidazole functionalities. PBI-co exhibits a very high room-temperature proton conductivity of 0.138 S cm–1, as measured by electrochemical impedance spectroscopy. PBI-co also demonstrates electromigration crossover mitigation under applied current densities up to 500 mA cm–2, and voltage pulses up to 1.4 V, while also inhibiting diffusion-driven vanadium crossover for over 20 days. Single-cell vanadium flow battery testing on post-functionalized PBI-co further confirms state-of-the-art battery performance with an ∼99.5% Coulombic efficiency at 100 mA cm–2 and an area-specific resistance of ∼20 mΩ cm2 lower than Nafion-212 membrane.

quote

GB/T 7714-2015 [1] Saheed Bukola, Ashlee Vise, Yuanshun Li, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.1c01318.
MLA [1] Saheed Bukola, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.1c01318.
APA [1] Saheed Bukola, Ashlee Vise, Yuanshun Li, Gabriel Goenaga, Thomas A. Zawodzinski, Jeffrey L. Blackburn, & Bryan Pivovar. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.1c01318
IEEE [1] Saheed Bukola, Ashlee Vise, Yuanshun Li, Gabriel Goenaga, Thomas A. Zawodzinski, Jeffrey L. Blackburn, and Bryan Pivovar, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.1c01318. keywords: {membrane;polybenzimidazole copolymer;proton transport;batteries;vanadium crossover}