Cyclodextrin Polymers with Nitrogen-Containing Tripodal Crosslinkers for Efficient PFAS Adsorption AITranslate
Abstract AITranslate
Per- and polyfluoroalkyl substances (PFAS) are widely used industrial chemicals that are of a great concern because of their pervasive presence in water resources and association with negative health effects. Crosslinked β-cyclodextrin-containing (β-CD) polymer adsorbents have shown promising performances for sequestering PFAS. Recently, installing amino groups into the crosslinkers of a β-CD polymer network improved the binding of many anionic PFAS, including short-chain and branched derivatives. However, the relative importance of the electrostatic interactions from the amino groups and the host-guest interactions within the cavity of the β-CD for PFAS binding are unclear. Herein, β-CD-based adsorbents crosslinked with tripodal crosslinkers containing three amino or amido groups are prepared with comparable physicochemical properties to investigate the respective roles of the crosslinker and β-CD in binding affinity and capacity for anionic PFAS. β-CD polymers containing amines showed superior removal for ten anionic PFAS compared to polymers containing amido groups. Both β-CD polymers have superior performance for perfluorooctanoic acid (PFOA) removal compared to activated carbons (ACs), consistent with β-CD:PFOA inclusion complexes playing an important role. Adsorbents containing amido groups showed low binding affinity and capacity for GenX, whereas the amine-functionalized polymer had outstanding affinity and capacity for GenX (KL = 8.8 × 104 M–1, QM = 222 mg g–1), underscoring the essential role of electrostatic interactions for removing short-chain and branched PFAS. The amine-containing β-CD polymer exhibited 100-fold higher affinity and twice the capacity (KL = 1.8 × 106 M–1, QM = 457 mg g–1) for PFOA compared to GenX, which are the highest reported values for β-CD polymers. These results highlight the synergistic effects of electrostatic interactions and host-guest interactions in β-CD polymers as important design criteria for efficient removal of anionic PFAS from water. This study further demonstrates broad tunability of crosslinked β-CD polymers and their promise as adsorbents for PFAS remediation.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsmaterialslett.0c00240
Chinese Library Classification Number:
Citation Information:
Per- and polyfluoroalkyl substances (PFAS) are widely used industrial chemicals that are of a great concern because of their pervasive presence in water resources and association with negative health effects. Crosslinked β-cyclodextrin-containing (β-CD) polymer adsorbents have shown promising performances for sequestering PFAS. Recently, installing amino groups into the crosslinkers of a β-CD polymer network improved the binding of many anionic PFAS, including short-chain and branched derivatives. However, the relative importance of the electrostatic interactions from the amino groups and the host-guest interactions within the cavity of the β-CD for PFAS binding are unclear. Herein, β-CD-based adsorbents crosslinked with tripodal crosslinkers containing three amino or amido groups are prepared with comparable physicochemical properties to investigate the respective roles of the crosslinker and β-CD in binding affinity and capacity for anionic PFAS. β-CD polymers containing amines showed superior removal for ten anionic PFAS compared to polymers containing amido groups. Both β-CD polymers have superior performance for perfluorooctanoic acid (PFOA) removal compared to activated carbons (ACs), consistent with β-CD:PFOA inclusion complexes playing an important role. Adsorbents containing amido groups showed low binding affinity and capacity for GenX, whereas the amine-functionalized polymer had outstanding affinity and capacity for GenX (KL = 8.8 × 104 M–1, QM = 222 mg g–1), underscoring the essential role of electrostatic interactions for removing short-chain and branched PFAS. The amine-containing β-CD polymer exhibited 100-fold higher affinity and twice the capacity (KL = 1.8 × 106 M–1, QM = 457 mg g–1) for PFOA compared to GenX, which are the highest reported values for β-CD polymers. These results highlight the synergistic effects of electrostatic interactions and host-guest interactions in β-CD polymers as important design criteria for efficient removal of anionic PFAS from water. This study further demonstrates broad tunability of crosslinked β-CD polymers and their promise as adsorbents for PFAS remediation.
quote
| GB/T 7714-2015 | [1] Anna Yang, Casey Ching, Maeghan Easler, et al. ACS Materials Letters, 2020(2). DOI:10.1021/acsmaterialslett.0c00240. |
| MLA | [1] Anna Yang, et al., ACS Materials Letters, no. 2, 2020, https://doi.org/10.1021/acsmaterialslett.0c00240. |
| APA | [1] Anna Yang, Casey Ching, Maeghan Easler, Damian E. Helbling, & William R. Dichtel. (2020). ACS Materials Letters(2). https://doi.org/10.1021/acsmaterialslett.0c00240 |
| IEEE | [1] Anna Yang, Casey Ching, Maeghan Easler, Damian E. Helbling, and William R. Dichtel, ACS Materials Letters, no. 2, 2020, doi: 10.1021/acsmaterialslett.0c00240. |