Antimicrobial Performance of Bioinspired PLA Fabricated via One-Step Plasma Etching with Silver and Copper AITranslate

Federal University of ABC (UFABC); Federal University of ABC (UFABC)
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Nanotechnology has been adopted to mimic a biological system to design artificial nanostructures with properties suitable for advanced applications. In this way, bioinspired bactericidal surfaces with surface nanostructured like insect wings display antimicrobial properties that undergo a physicomechanical mechanism that disrupts the microbial cells, inhibiting their growth and proliferation. Herein, we describe a method to design nanocone patterns on the surface of poly(lactic acid) (PLA) via one step of argon plasma etching in the presence of silver and copper. In this contribution, PLA with nanocone patterns were successfully obtained using 30 and 60 s of plasma etching, mimicking the surface of cicada wings that avoids the attachment of Escherichia coli, which is suitable for self-disinfectant medical devices. However, the plasma etching during 120 s generates a maze-like topographical surface with nanoholes that hampers both the adhesion and proliferation of bacteria on the PLA surface, which are important functional characteristics to fabricate self-disinfecting personal protection equipment for healthcare professionals in hospital environments subject to a wide variety of pathogenic microorganisms that adhere and proliferate on the material surfaces.

KeyWords AITranslate

silver surface nanotopography copper poly(lactic acid)
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c01043

Chinese Library Classification Number:

Citation Information:

Nanotechnology has been adopted to mimic a biological system to design artificial nanostructures with properties suitable for advanced applications. In this way, bioinspired bactericidal surfaces with surface nanostructured like insect wings display antimicrobial properties that undergo a physicomechanical mechanism that disrupts the microbial cells, inhibiting their growth and proliferation. Herein, we describe a method to design nanocone patterns on the surface of poly(lactic acid) (PLA) via one step of argon plasma etching in the presence of silver and copper. In this contribution, PLA with nanocone patterns were successfully obtained using 30 and 60 s of plasma etching, mimicking the surface of cicada wings that avoids the attachment of Escherichia coli, which is suitable for self-disinfectant medical devices. However, the plasma etching during 120 s generates a maze-like topographical surface with nanoholes that hampers both the adhesion and proliferation of bacteria on the PLA surface, which are important functional characteristics to fabricate self-disinfecting personal protection equipment for healthcare professionals in hospital environments subject to a wide variety of pathogenic microorganisms that adhere and proliferate on the material surfaces.

quote

GB/T 7714-2015 [1] Daniel J. da Silva, Derval S. Rosa. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c01043.
MLA [1] Daniel J. da Silva, and Derval S. Rosa. ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c01043.
APA [1] Daniel J. da Silva, & Derval S. Rosa. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c01043