Fruit Peel-Inspired Super-Stable Ionic Organohydrogel Electronics with Dense Hydrophobic Skin AITranslate
Abstract AITranslate
Hydrogels are easily dehydrated during use and storage, making it difficult to maintain structural and performance stability, which greatly reduces their application value as wearable devices. Inspired by the structure of fruit, an ionic organohydrogel core containing Ca2+ and glycerol was first fabricated, and then, stearic acid (STA) was rivetted on the organohydrogel surface through (3-aminopropyl) triethoxysilane to obtain a dense hydrophobic coating (100 μm). The organohydrogel with hydrophobic skin presented better water spreading resistance and mechanical strength. In addition to the moisturizing effect of Ca2+ and glycerol, the skin also further blocks the contact between the organohydrogel and the air, thereby significantly enhancing the anti-dryness of the organohydrogel. Therefore, this organohydrogel has extremely outstanding structural, strength, and electrical conductivity stability. The developed strain sensor based on this organohydrogel can realize human motion monitoring capability at ultra-low temperature. This design idea, which combines multiple anti-drying mechanisms, has great expansion value for other gels suitable for various application scenarios.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.2c00160
Chinese Library Classification Number:
Citation Information:
Hydrogels are easily dehydrated during use and storage, making it difficult to maintain structural and performance stability, which greatly reduces their application value as wearable devices. Inspired by the structure of fruit, an ionic organohydrogel core containing Ca2+ and glycerol was first fabricated, and then, stearic acid (STA) was rivetted on the organohydrogel surface through (3-aminopropyl) triethoxysilane to obtain a dense hydrophobic coating (100 μm). The organohydrogel with hydrophobic skin presented better water spreading resistance and mechanical strength. In addition to the moisturizing effect of Ca2+ and glycerol, the skin also further blocks the contact between the organohydrogel and the air, thereby significantly enhancing the anti-dryness of the organohydrogel. Therefore, this organohydrogel has extremely outstanding structural, strength, and electrical conductivity stability. The developed strain sensor based on this organohydrogel can realize human motion monitoring capability at ultra-low temperature. This design idea, which combines multiple anti-drying mechanisms, has great expansion value for other gels suitable for various application scenarios.
quote
| GB/T 7714-2015 | [1] Jing Yu, Qinhua Wang, Xiaofeng Pan, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c00160. |
| MLA | [1] Jing Yu, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c00160. |
| APA | [1] Jing Yu, Qinhua Wang, Xiaofeng Pan, Xiaojuan Ma, Shilin Cao, & Yonghao Ni. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c00160 |
| IEEE | [1] Jing Yu, Qinhua Wang, Xiaofeng Pan, Xiaojuan Ma, Shilin Cao, and Yonghao Ni, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c00160. keywords: {antidryness gel;organohydrogel;polymer coating;hydrophobic skin;ionic conductive;strain sensor} |