daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Conjugated Polyelectrolyte Photocatalysts: The Use of Zwitterionic Side Groups for High Performance AITranslate

Shanghai Normal University; Shanghai Normal University; Zhengzhou University of Technology; Shanghai Institute of Organic Chemistry; Shanghai Institute of Organic Chemistry; Zhengzhou University of Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Conjugated polyelectrolytes have emerged as a class of organic photocatalysts for light-driven hydrogen production from water due to their photoactive conjugated backbones and hydrophilic ionic side chains. However, compared to well-documented anionic and cationic side chains, zwitterionic side chains have been rarely reported. Herein, based on the thiophene (T)-dibenzo[b,d]thiophene sulfone (DBTSO) donor–acceptor backbone, a zwitterionic side chain-modified polymer PTDBTSO-ZS as well as an alkylated polymer PTDBTSO-C6, a cationic polymer PTDBTSO-QA, and an anionic polymer PTDBTSO-SS has been synthesized and studied. It was found that zwitterionic side chain modification can endow the polymer with good hydrophilicity, a large proportion of excited energy used for charge separation, long-lived excitons, reinforced interchain interactions, and the smallest interfacial charge transfer resistance. Consequently, PTDBTSO-ZS behaves the best in the family with a hydrogen evolution rate of 55.2 mmol g–1 h–1 under full-arc Xe light irradiation, which is 1.4-, 1.7-, and 10.0-fold as compared to those of PTDBTSO-QA, PTDBTSO-SS, and PTDBTSO-C6, respectively.

KeyWords AITranslate

water splitting photocatalytic hydrogen evolution organic photocatalysts conjugated polyelectrolytes zwitterionic side chains
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c01665

Chinese Library Classification Number:

Citation Information:

Conjugated polyelectrolytes have emerged as a class of organic photocatalysts for light-driven hydrogen production from water due to their photoactive conjugated backbones and hydrophilic ionic side chains. However, compared to well-documented anionic and cationic side chains, zwitterionic side chains have been rarely reported. Herein, based on the thiophene (T)-dibenzo[b,d]thiophene sulfone (DBTSO) donor–acceptor backbone, a zwitterionic side chain-modified polymer PTDBTSO-ZS as well as an alkylated polymer PTDBTSO-C6, a cationic polymer PTDBTSO-QA, and an anionic polymer PTDBTSO-SS has been synthesized and studied. It was found that zwitterionic side chain modification can endow the polymer with good hydrophilicity, a large proportion of excited energy used for charge separation, long-lived excitons, reinforced interchain interactions, and the smallest interfacial charge transfer resistance. Consequently, PTDBTSO-ZS behaves the best in the family with a hydrogen evolution rate of 55.2 mmol g–1 h–1 under full-arc Xe light irradiation, which is 1.4-, 1.7-, and 10.0-fold as compared to those of PTDBTSO-QA, PTDBTSO-SS, and PTDBTSO-C6, respectively.

quote

GB/T 7714-2015 [1] Qian Li, KangHua Li, LiNa Liu, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c01665.
MLA [1] Qian Li, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c01665.