Mechanically conditioned multilayered angle-ply collagen scaffolds promote annulus fibrosus regeneration AITranslate

Soochow University; Soochow University; Soochow University; Soochow University; Soochow University; Soochow University; Affiliated Hospital of Nantong University; Soochow University
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Annulus fibrosus (AF) injury, as a result of intervertebral disk degeneration (IVDD) or herniation, is very difficult to heal due to its avascular characteristics. Tissue engineering strategies have become increasingly promising to treat IVDD. However, in light of the fact that AF displays an anisotropic microstructure that results in gradient mechanical properties, fabrication of tissue engineered AF remains challenging. In this study, we fabricated micropatterned collagen scaffolds with angle-ply structure mimicking the microstructural features of AF. Following that, we cultured bone marrow mesenchymal stromal cells (BMSCs) in the scaffolds and applied cyclic stretching to them to mechanically stimulate the cells. We found that aligned cells under mechanical loading showed elevated expression of matrix anabolism-related genes and proteins. Further studies indicated that Caveolin-1 (CAV1) might mediate the nuclear translocation of Yes-associated protein (YAP) in response to external mechanical cues of microgroove-patterned membranes and mechanical loading. Micropatterned collagen membranes, with cells aligning at ±30° along the longitudinal dimension, were rolled up together to form an angle-ply and multilayered tissue. After being implanted into the caudal vertebra in a rat model for 4 weeks, biomimetic tissues showed improved restoration of the disk. In general, our biomimetic collagen membranes exhibit great potential in terms of AF regeneration, with AF-like heterogeneous microstructures that satisfy the biomechanical property of the native disk. Graphical abstract Preparation of the multilayer and angle-ply cell-collagen construct and its implantation in a rat model of diskectomy. Download : Download high-res image (207KB) Download : Download full-size image

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.apmt.2023.101751

Chinese Library Classification Number:

Citation Information:

Annulus fibrosus (AF) injury, as a result of intervertebral disk degeneration (IVDD) or herniation, is very difficult to heal due to its avascular characteristics. Tissue engineering strategies have become increasingly promising to treat IVDD. However, in light of the fact that AF displays an anisotropic microstructure that results in gradient mechanical properties, fabrication of tissue engineered AF remains challenging. In this study, we fabricated micropatterned collagen scaffolds with angle-ply structure mimicking the microstructural features of AF. Following that, we cultured bone marrow mesenchymal stromal cells (BMSCs) in the scaffolds and applied cyclic stretching to them to mechanically stimulate the cells. We found that aligned cells under mechanical loading showed elevated expression of matrix anabolism-related genes and proteins. Further studies indicated that Caveolin-1 (CAV1) might mediate the nuclear translocation of Yes-associated protein (YAP) in response to external mechanical cues of microgroove-patterned membranes and mechanical loading. Micropatterned collagen membranes, with cells aligning at ±30° along the longitudinal dimension, were rolled up together to form an angle-ply and multilayered tissue. After being implanted into the caudal vertebra in a rat model for 4 weeks, biomimetic tissues showed improved restoration of the disk. In general, our biomimetic collagen membranes exhibit great potential in terms of AF regeneration, with AF-like heterogeneous microstructures that satisfy the biomechanical property of the native disk. Graphical abstract Preparation of the multilayer and angle-ply cell-collagen construct and its implantation in a rat model of diskectomy. Download : Download high-res image (207KB) Download : Download full-size image

quote

GB/T 7714-2015 [1] Weidong Zhang, Huan Wang, Genglei Chu, et al. Applied Materials Today, 2023(31). DOI:10.1016/j.apmt.2023.101751.
MLA [1] Weidong Zhang, et al., Applied Materials Today, no. 31, 2023, https://doi.org/10.1016/j.apmt.2023.101751.
APA [1] Weidong Zhang, Huan Wang, Genglei Chu, Li Yu, Feng Han, Qifan Yu, Youhua Wang, & Bin Li. (2023). Applied Materials Today(31). https://doi.org/10.1016/j.apmt.2023.101751
IEEE [1] Weidong Zhang, Huan Wang, Genglei Chu, Li Yu, Feng Han, Qifan Yu, Youhua Wang, and Bin Li, Applied Materials Today, no. 31, 2023, doi: 10.1016/j.apmt.2023.101751.