Partially Biobased Block Copolymers Derived from Phenol and Butanol for High-Performance Elastomers and Pressure-Sensitive Adhesives AITranslate
Abstract AITranslate
Upcycling renewable resources into value-added products has shown substantial promise for producing sustainable polymers and reducing environmental pollution. To achieve this, careful and cost-effective selections of monomers derived from bioresources are critical. We herein report ABA-type triblock copolymers that partly contain phenyl acrylate and n-butyl acrylate, which could be derived from natural resources, such as lignin (for phenol) and microorganisms (for n-butanol). A hard block (“A” block) is first formed using phenyl acrylate and styrene with a bifunctional reversible addition–fragmentation chain-transfer agent, followed by the incorporation of n-butyl acrylate to form a soft block (“B” block) in the middle. The biomass contents are calculated to range from 32 to 53%. By simply altering the feeding ratios of these monomers, we have developed materials that exhibit excellent properties, ranging from elastomers to pressure-sensitive adhesives (PSAs). For example, one of the synthesized polymers indicates a Young’s modulus of 106 MPa and a toughness of 15 MJ/m3, outperforming those obtained from commercial petrochemical-based elastomers. Additionally, some of the copolymers exhibited PSA properties that surpass those of commercial packaging tapes and glue sticks on a certain substrate. The Dahlquist criteria and viscoelastic window indicate great promise for these biobased polymers as PSAs.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.3c01053
Chinese Library Classification Number:
Citation Information:
Upcycling renewable resources into value-added products has shown substantial promise for producing sustainable polymers and reducing environmental pollution. To achieve this, careful and cost-effective selections of monomers derived from bioresources are critical. We herein report ABA-type triblock copolymers that partly contain phenyl acrylate and n-butyl acrylate, which could be derived from natural resources, such as lignin (for phenol) and microorganisms (for n-butanol). A hard block (“A” block) is first formed using phenyl acrylate and styrene with a bifunctional reversible addition–fragmentation chain-transfer agent, followed by the incorporation of n-butyl acrylate to form a soft block (“B” block) in the middle. The biomass contents are calculated to range from 32 to 53%. By simply altering the feeding ratios of these monomers, we have developed materials that exhibit excellent properties, ranging from elastomers to pressure-sensitive adhesives (PSAs). For example, one of the synthesized polymers indicates a Young’s modulus of 106 MPa and a toughness of 15 MJ/m3, outperforming those obtained from commercial petrochemical-based elastomers. Additionally, some of the copolymers exhibited PSA properties that surpass those of commercial packaging tapes and glue sticks on a certain substrate. The Dahlquist criteria and viscoelastic window indicate great promise for these biobased polymers as PSAs.
quote
| GB/T 7714-2015 | [1] Soyeon Kim, Byungjin Koo. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c01053. |
| MLA | [1] Soyeon Kim, and Byungjin Koo. ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c01053. |
| APA | [1] Soyeon Kim, & Byungjin Koo. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c01053 |
| IEEE | [1] Soyeon Kim and Byungjin Koo, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c01053. keywords: {biobased monomer;triblock copolymer;lignin;elastomer;pressuresensitive adhesive} |