Transformation of a Hydrazone-Linked Covalent Organic Framework into a Highly Stable Hydrazide-Linked One AITranslate
Abstract AITranslate
The development of covalent organic frameworks (COFs) with advanced linkages and exceptional chemical stability is of importance but remains a challenge. Herein, a hydrazone-linked COF (hydrazone-MTH-TFPB COF) was converted through mild oxidation into a hydrazide-linked one (hydrazide-MTH-TFPB COF). The hydrazide-linked COF exhibited high crystallinity, permanent porosity, and superb chemical stability in boiling water, strong acid, and strong base conditions. Moreover, hydrazide-MTH-TFPB COF displayed superior iodine uptake relative to hydrazone-MTH-TFPB COF, presumably due to the favorable interaction between iodine molecules and hydrazide moieties in the oxidized COF. This work delineates a facile approach for accessing hydrazide-linked COFs that are otherwise difficult to crystallize de novo.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.2c00543
Chinese Library Classification Number:
Citation Information:
The development of covalent organic frameworks (COFs) with advanced linkages and exceptional chemical stability is of importance but remains a challenge. Herein, a hydrazone-linked COF (hydrazone-MTH-TFPB COF) was converted through mild oxidation into a hydrazide-linked one (hydrazide-MTH-TFPB COF). The hydrazide-linked COF exhibited high crystallinity, permanent porosity, and superb chemical stability in boiling water, strong acid, and strong base conditions. Moreover, hydrazide-MTH-TFPB COF displayed superior iodine uptake relative to hydrazone-MTH-TFPB COF, presumably due to the favorable interaction between iodine molecules and hydrazide moieties in the oxidized COF. This work delineates a facile approach for accessing hydrazide-linked COFs that are otherwise difficult to crystallize de novo.
quote
| GB/T 7714-2015 | [1] YiXuan Yang, XiHao Tang, JiaLin Wu, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c00543. |
| MLA | [1] YiXuan Yang, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c00543. |
| APA | [1] YiXuan Yang, XiHao Tang, JiaLin Wu, ZhaoYi Dong, YiLun Yan, ShengRun Zheng, Jun Fan, Xinle Li, Songliang Cai, & WeiGuang Zhang. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c00543 |
| IEEE | [1] YiXuan Yang, XiHao Tang, JiaLin Wu, ZhaoYi Dong, YiLun Yan, ShengRun Zheng, Jun Fan, Xinle Li, Songliang Cai, and WeiGuang Zhang, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c00543. keywords: {covalent organic frameworks;hydrazonelinked COF;hydrazidelinked COF;linkage transformation;robust COF;iodine adsorption} |