Abstract AITranslate

The development of advanced energy storage and conversion technology is a significant global concern, in which the innovation in materials would feature prominently for next-generation energy devices. Graphene, as a typical two-dimensional (2D) material, is acknowledged to have a significant impact on today’s energy-storage/conversion evolution. The effectuation for future energy landscape should still enlist alternative 2D materials with high electrochemical activity and energy density. As a group of 2D nanomaterials, metallene is considered as a potential candidate because of its fantastic physicochemical properties. In this Review, the structures, synthesis strategies, and properties of various metallenes are systematically introduced. The research progress and latest achievements in the energy field are reviewed, including Li-/Na-/K-ion batteries, Li–S batteries, solar cells, and typical catalytic processes (i.e., CO2/N2/O2 reduction reaction, hydrogen/oxygen evolution reaction, etc.). Besides, the challenges of miscellaneous energy storage/conversion devices and the advantages of applications of metallenes are discussed and compared. Finally, the development prospects are provided as suggested guidelines for future researches.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsmaterialslett.0c00280

Chinese Library Classification Number:

Citation Information:

The development of advanced energy storage and conversion technology is a significant global concern, in which the innovation in materials would feature prominently for next-generation energy devices. Graphene, as a typical two-dimensional (2D) material, is acknowledged to have a significant impact on today’s energy-storage/conversion evolution. The effectuation for future energy landscape should still enlist alternative 2D materials with high electrochemical activity and energy density. As a group of 2D nanomaterials, metallene is considered as a potential candidate because of its fantastic physicochemical properties. In this Review, the structures, synthesis strategies, and properties of various metallenes are systematically introduced. The research progress and latest achievements in the energy field are reviewed, including Li-/Na-/K-ion batteries, Li–S batteries, solar cells, and typical catalytic processes (i.e., CO2/N2/O2 reduction reaction, hydrogen/oxygen evolution reaction, etc.). Besides, the challenges of miscellaneous energy storage/conversion devices and the advantages of applications of metallenes are discussed and compared. Finally, the development prospects are provided as suggested guidelines for future researches.

quote

GB/T 7714-2015 [1] Yaoda Liu, Khang Ngoc Dinh, Zhengfei Dai, et al. ACS Materials Letters, 2020(2). DOI:10.1021/acsmaterialslett.0c00280.
MLA [1] Yaoda Liu, et al., ACS Materials Letters, no. 2, 2020, https://doi.org/10.1021/acsmaterialslett.0c00280.
APA [1] Yaoda Liu, Khang Ngoc Dinh, Zhengfei Dai, & Qingyu Yan. (2020). ACS Materials Letters(2). https://doi.org/10.1021/acsmaterialslett.0c00280
IEEE [1] Yaoda Liu, Khang Ngoc Dinh, Zhengfei Dai, and Qingyu Yan, ACS Materials Letters, no. 2, 2020, doi: 10.1021/acsmaterialslett.0c00280.