daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

4D Printing of MXene Composites for Deployable Actuating Structures AITranslate

University of Toronto; University of Toronto; University of Toronto;Security & Disruptive Technologies Research Centre, Division of Emerging Technologies; University of Toronto
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The development of innovative materials for three-dimensional (3D) printing is creating potential opportunities for advancements in additive manufacturing (AM) technologies, including in four-dimensional (4D) printing. Through the creation of next-generation shape memory polymer composites (SMPCs), printed parts can now be bestowed with increased functionalities including the ability to transform their shape, acting as smart actuators that respond to the stimuli around them. These materials are of great interest for development of soft robotic systems, which can be quickly and affordably manufactured. In this work, a SMPC consisting of a TPU:PLA polymer blend system with embedded MXene (Ti3C2) flakes is fabricated and evaluated. The mechanical, thermal, and morphological properties prove to be greatly improved with the addition of MXene at 0.5 wt %. At higher loadings of 2 wt % MXene, the composite shows superb shape memory effect results in fast recovery to ∼98% its original position in under 14 s. Rheological behavior and thermal properties were evaluated, followed by 3D printing using material extrusion. Results show great potential of MXene-loaded composites for fast shape memory actuation in 3D/4D printed structures. The potential of such composites is demonstrated through several printed designs, which show large deformation suitable for deployable structures.

KeyWords AITranslate

shape memory materials 4D printing responsive structures MXene deployable structures
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c01192

Chinese Library Classification Number:

Citation Information:

The development of innovative materials for three-dimensional (3D) printing is creating potential opportunities for advancements in additive manufacturing (AM) technologies, including in four-dimensional (4D) printing. Through the creation of next-generation shape memory polymer composites (SMPCs), printed parts can now be bestowed with increased functionalities including the ability to transform their shape, acting as smart actuators that respond to the stimuli around them. These materials are of great interest for development of soft robotic systems, which can be quickly and affordably manufactured. In this work, a SMPC consisting of a TPU:PLA polymer blend system with embedded MXene (Ti3C2) flakes is fabricated and evaluated. The mechanical, thermal, and morphological properties prove to be greatly improved with the addition of MXene at 0.5 wt %. At higher loadings of 2 wt % MXene, the composite shows superb shape memory effect results in fast recovery to ∼98% its original position in under 14 s. Rheological behavior and thermal properties were evaluated, followed by 3D printing using material extrusion. Results show great potential of MXene-loaded composites for fast shape memory actuation in 3D/4D printed structures. The potential of such composites is demonstrated through several printed designs, which show large deformation suitable for deployable structures.

quote

GB/T 7714-2015 [1] Kyra McLellan, Terek Li, YuChen Sun, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c01192.
MLA [1] Kyra McLellan, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c01192.
APA [1] Kyra McLellan, Terek Li, YuChen Sun, Michael B. Jakubinek, & Hani E. Naguib. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c01192
IEEE [1] Kyra McLellan, Terek Li, YuChen Sun, Michael B. Jakubinek, and Hani E. Naguib, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c01192. keywords: {shape memory materials;4D printing;responsive structures;MXene;deployable structures}