MoS2 Polymorphic Engineering Enhances Selectivity in the Electrochemical Reduction of Nitrogen to Ammonia AITranslate
Abstract AITranslate
The electrochemical N2 reduction reaction (NRR) offers a direct pathway to produce NH3 from renewable energy. However, aqueous NRR suffers from both low Faradaic efficiency (FE) and low yield rate. The main reason is the more favored H+ reduction to H2 in aqueous electrolytes. Here we demonstrate a highly selective Ru/MoS2 NRR catalyst on which the MoS2 polymorphs can be controlled to suppress H+ reduction. A NRR FE as high as 17.6% and NH3 yield rate of 1.14 × 10–10 mol cm–2 s–1 are demonstrated at 50 °C. Theoretical evidence supports a hypothesis that the high NRR activity originates from the synergistic interplay between the Ru clusters as N2 binding sites and nearby isolated S-vacancies on the 2H-MoS2 as centers for hydrogenation; this supports formation of NH3 at the Ru/2H-MoS2 interface.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.8b02257
Chinese Library Classification Number:
Citation Information:
The electrochemical N2 reduction reaction (NRR) offers a direct pathway to produce NH3 from renewable energy. However, aqueous NRR suffers from both low Faradaic efficiency (FE) and low yield rate. The main reason is the more favored H+ reduction to H2 in aqueous electrolytes. Here we demonstrate a highly selective Ru/MoS2 NRR catalyst on which the MoS2 polymorphs can be controlled to suppress H+ reduction. A NRR FE as high as 17.6% and NH3 yield rate of 1.14 × 10–10 mol cm–2 s–1 are demonstrated at 50 °C. Theoretical evidence supports a hypothesis that the high NRR activity originates from the synergistic interplay between the Ru clusters as N2 binding sites and nearby isolated S-vacancies on the 2H-MoS2 as centers for hydrogenation; this supports formation of NH3 at the Ru/2H-MoS2 interface.
quote
| GB/T 7714-2015 | [1] Bryan H. R. Suryanto, Dabin Wang, Luis Miguel Azofra, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.8b02257. |
| MLA | [1] Bryan H. R. Suryanto, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.8b02257. |
| APA | [1] Bryan H. R. Suryanto, Dabin Wang, Luis Miguel Azofra, Moussab Harb, Luigi Cavallo, Rouhollah Jalili, David R. G. Mitchell, Manjunath Chatti, & Douglas R. MacFarlane. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.8b02257 |
| IEEE | [1] Bryan H. R. Suryanto, Dabin Wang, Luis Miguel Azofra, Moussab Harb, Luigi Cavallo, Rouhollah Jalili, David R. G. Mitchell, Manjunath Chatti, and Douglas R. MacFarlane, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.8b02257. |