Synthesis of Interface-Driven Tunable Bandgap Metal Oxides AITranslate

Iowa State University; Iowa State University; Iowa State University; Tianjin University; Iowa State University; Tianjin University; Iowa State University; Iowa State University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Mixed bandgap and bandgap tunability in semiconductors is critical in expanding their use. Composition alterations through single-crystal epitaxial growth and the formation of multilayer tandem structures are often employed to achieve mixed bandgaps, albeit with limited tunability. Herein, self-assembled one-dimensional coordination polymers provide facile synthons and templates for graphitic C-doped mesoporous oxides, gC-β-Ga2O3 or gC-In2O3 via controlled oxidative ligand ablation. These materials have mixed bandgaps and colors, depending on amount of gC present. The carbon/oxide interface leads to induced gap states, hence, a stoichiometrically tunable band structure. Structurally, a multiscale porous network percolating throughout the material is realized. The nature of the heat treatment and the top-down process allows for facile tunability and the formation of mixed bandgap metal oxides through controlled carbon deposition. As a proof of concept, gC-β-Ga2O3 was utilized as a photocatalyst for CO2 reduction, which demonstrated excellent conversion rates into CH4 and CO.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsmaterialslett.0c00251

Chinese Library Classification Number:

Citation Information:

Mixed bandgap and bandgap tunability in semiconductors is critical in expanding their use. Composition alterations through single-crystal epitaxial growth and the formation of multilayer tandem structures are often employed to achieve mixed bandgaps, albeit with limited tunability. Herein, self-assembled one-dimensional coordination polymers provide facile synthons and templates for graphitic C-doped mesoporous oxides, gC-β-Ga2O3 or gC-In2O3 via controlled oxidative ligand ablation. These materials have mixed bandgaps and colors, depending on amount of gC present. The carbon/oxide interface leads to induced gap states, hence, a stoichiometrically tunable band structure. Structurally, a multiscale porous network percolating throughout the material is realized. The nature of the heat treatment and the top-down process allows for facile tunability and the formation of mixed bandgap metal oxides through controlled carbon deposition. As a proof of concept, gC-β-Ga2O3 was utilized as a photocatalyst for CO2 reduction, which demonstrated excellent conversion rates into CH4 and CO.

quote

GB/T 7714-2015 [1] Boyce S. Chang, Andrew Martin, Brijith Thomas, et al. ACS Materials Letters, 2020(2). DOI:10.1021/acsmaterialslett.0c00251.
MLA [1] Boyce S. Chang, et al., ACS Materials Letters, no. 2, 2020, https://doi.org/10.1021/acsmaterialslett.0c00251.
APA [1] Boyce S. Chang, Andrew Martin, Brijith Thomas, Ang Li, Rick W. Dorn, Jinlong Gong, Aaron J. Rossini, & Martin M. Thuo. (2020). ACS Materials Letters(2). https://doi.org/10.1021/acsmaterialslett.0c00251
IEEE [1] Boyce S. Chang, Andrew Martin, Brijith Thomas, Ang Li, Rick W. Dorn, Jinlong Gong, Aaron J. Rossini, and Martin M. Thuo, ACS Materials Letters, no. 2, 2020, doi: 10.1021/acsmaterialslett.0c00251.