Grain Boundaries of Self-Assembled Porous Polymer Films for Unclonable Anti-Counterfeiting AITranslate

Zhejiang University; Zhejiang University; Zhejiang University; Zhejiang University; Zhejiang University; Zhejiang University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Grain boundaries widely exist in 2-D materials, and they are often considered as defects harming the physicochemical properties of materials. Here, we report unclonable anti-counterfeiting films based on the grain boundaries of patterned porous structures. The porous films are prepared from hydroxyl-end-functionalized polystyrene (OH-PS), polystyrene-block-poly(N,N-dimethylaminoethly methacrylate) (PS-b-PDMAEMA), and cyclic polystyrene (c-PS) via a typical breath figure process, during which the evaporation of solvents provides enough instability and promises the uniqueness of surface grain boundaries. The anti-counterfeiting tags are convenient to be authenticated by portable devices. The self-assembly nature of the arrays endows the films with an extremely high encoding capacity. Moreover, the present anti-counterfeiting films are configurable, transparent, flexible, and aesthetically appealing to adapt to various applications. This work demonstrates highly secure unclonable anti-counterfeiting films and provides new understandings to grain boundaries of 2-D materials.

KeyWords AITranslate

grain boundaries breath figure anticounterfeiting physical unclonable function high encoding capacity
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.8b00031

Chinese Library Classification Number:

Citation Information:

Grain boundaries widely exist in 2-D materials, and they are often considered as defects harming the physicochemical properties of materials. Here, we report unclonable anti-counterfeiting films based on the grain boundaries of patterned porous structures. The porous films are prepared from hydroxyl-end-functionalized polystyrene (OH-PS), polystyrene-block-poly(N,N-dimethylaminoethly methacrylate) (PS-b-PDMAEMA), and cyclic polystyrene (c-PS) via a typical breath figure process, during which the evaporation of solvents provides enough instability and promises the uniqueness of surface grain boundaries. The anti-counterfeiting tags are convenient to be authenticated by portable devices. The self-assembly nature of the arrays endows the films with an extremely high encoding capacity. Moreover, the present anti-counterfeiting films are configurable, transparent, flexible, and aesthetically appealing to adapt to various applications. This work demonstrates highly secure unclonable anti-counterfeiting films and provides new understandings to grain boundaries of 2-D materials.

quote

GB/T 7714-2015 [1] BaiHeng Wu, Chao Zhang, Ning Zheng, et al. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.8b00031.
MLA [1] BaiHeng Wu, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.8b00031.
APA [1] BaiHeng Wu, Chao Zhang, Ning Zheng, LianWei Wu, ZhiKang Xu, & LingShu Wan. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.8b00031
IEEE [1] BaiHeng Wu, Chao Zhang, Ning Zheng, LianWei Wu, ZhiKang Xu, and LingShu Wan, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.8b00031. keywords: {grain boundaries;breath figure;anticounterfeiting;physical unclonable function;high encoding capacity}