daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Mg-ion storage materials based on MnO2 frameworks AITranslate

Tohoku University; Tohoku University; Tohoku University; Tohoku University
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

A wide variety of crystal structures for MnO2, so-called polymorphs, is promising for basic frameworks of cathode materials in next-generation batteries such as Mg rechargeable batteries. In this short review, we summarize recent progress on MnO2-based cathode materials for Mg rechargeable batteries, especially focusing on the structures of α-MnO2 and λ-MnO2 to discuss the criteria for achieving topotactic reactions during magnesiation. In contrast to adequately stable α-MnO2, spinel-structured λ-MnO2 is unstable at elevated temperatures around 150 °C; however, its stability can be significantly improved by materials design. Here, we introduce as a successful example that defect spinel ZnMnO3 exhibits long-term cycle performance even at 150 °C with high potential and capacity.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.coelec.2023.101209

Chinese Library Classification Number:

Citation Information:

A wide variety of crystal structures for MnO2, so-called polymorphs, is promising for basic frameworks of cathode materials in next-generation batteries such as Mg rechargeable batteries. In this short review, we summarize recent progress on MnO2-based cathode materials for Mg rechargeable batteries, especially focusing on the structures of α-MnO2 and λ-MnO2 to discuss the criteria for achieving topotactic reactions during magnesiation. In contrast to adequately stable α-MnO2, spinel-structured λ-MnO2 is unstable at elevated temperatures around 150 °C; however, its stability can be significantly improved by materials design. Here, we introduce as a successful example that defect spinel ZnMnO3 exhibits long-term cycle performance even at 150 °C with high potential and capacity.

quote

GB/T 7714-2015 [1] Kohei Shimokawa, Takuya Hatakeyama, Hongyi Li, et al. Current Opinion in Electrochemistry, 2023(38). DOI:10.1016/j.coelec.2023.101209.
MLA [1] Kohei Shimokawa, et al., Current Opinion in Electrochemistry, no. 38, 2023, https://doi.org/10.1016/j.coelec.2023.101209.
APA [1] Kohei Shimokawa, Takuya Hatakeyama, Hongyi Li, & Tetsu Ichitsubo. (2023). Current Opinion in Electrochemistry(38). https://doi.org/10.1016/j.coelec.2023.101209