Theory-Driven Design and Targeting Synthesis of a Highly-Conjugated Basal-Plane 2D Covalent Organic Framework for Metal-Free Electrocatalytic OER AITranslate

Harbin University of Science and Technology; Harbin University of Science and Technology; Harbin University of Science and Technology; Heilongjiang University; Harbin University of Science and Technology; Harbin University of Science and Technology; Harbin University of Science and Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

It is a great challenge to obtain oriented design and synthesis of new two-dimensional covalent organic frameworks (2D-COFs) with proper CN stoichiometry, N position, and band structures as specific electrocatalysts. Driven by density functional theory (DFT) calculations, we designed and synthesized a new phenazine-linked 2D-COF (COF-C4N) by solvothermal reaction of triphenylenehexamine (TPHA) and hexaketocyclohexane (HKH). Structural analysis confirmed that COF-C4N possesses an ordered crystalline structure with a highly conjugated basal plane and better stability. COF-C4N exhibited OER performance with a low overpotential of 349 mV at 10 mA cm–2 and a Tafel slope of 64 mV dec–1. A combination of theoretical and experimental studies revealed that better OER performance is attributed to better crystallinity and stability, an appropriate band gap, and an N position that promotes the formation of C active sites around N atoms. The strategy of theory-driven design and targeting synthesis of 2D-COFs for OER may provide a new way to further develop metal-free materials for clean energy application.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.9b01691

Chinese Library Classification Number:

Citation Information:

It is a great challenge to obtain oriented design and synthesis of new two-dimensional covalent organic frameworks (2D-COFs) with proper CN stoichiometry, N position, and band structures as specific electrocatalysts. Driven by density functional theory (DFT) calculations, we designed and synthesized a new phenazine-linked 2D-COF (COF-C4N) by solvothermal reaction of triphenylenehexamine (TPHA) and hexaketocyclohexane (HKH). Structural analysis confirmed that COF-C4N possesses an ordered crystalline structure with a highly conjugated basal plane and better stability. COF-C4N exhibited OER performance with a low overpotential of 349 mV at 10 mA cm–2 and a Tafel slope of 64 mV dec–1. A combination of theoretical and experimental studies revealed that better OER performance is attributed to better crystallinity and stability, an appropriate band gap, and an N position that promotes the formation of C active sites around N atoms. The strategy of theory-driven design and targeting synthesis of 2D-COFs for OER may provide a new way to further develop metal-free materials for clean energy application.

quote

GB/T 7714-2015 [1] Chunhua Yang, ZhaoDi Yang, Hong Dong, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.9b01691.
MLA [1] Chunhua Yang, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.9b01691.
APA [1] Chunhua Yang, ZhaoDi Yang, Hong Dong, Ning Sun, Yang Lu, FengMing Zhang, & Guiling Zhang. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.9b01691
IEEE [1] Chunhua Yang, ZhaoDi Yang, Hong Dong, Ning Sun, Yang Lu, FengMing Zhang, and Guiling Zhang, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.9b01691.