daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Preparation of Random Polymers by Copolymerization of Rigid-Twisted Spirobiindane with Poly(aryl isatin) for High-Performance Anion Exchange Membranes AITranslate

Northeastern University; Northeastern University; Northeastern University; Northeastern University; Northeastern University;Shandong Province Linyi Ecological Environment Monitoring Center, Linyi 276000; Northeastern University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Designing the packing of polymer chains with reasonable fraction free volume (FFV) is regarded as an effective way to improve the conductivity of polymer-based membranes. We synthesize random polymers by copolymerization of bulky rigid-twisted spirobiindane, isatin, and one of the joint groups p-terphenyl, biphenyl, and 1,2-diphenylethane. The polycondensation reaction is catalyzed by trifluoromethanesulfonic acid. The introduced spirobiindane segments enlarge the distance of polymer chains and increase the FFV of the membrane. The formation of the microphase separation structure is evidenced according to the results of transmission electron microscopy and atomic force microscopy. As a result, a hydroxide conductivity of 126.7 mS cm–1 is achieved at 80 °C by the poly(spirobiindane diphenyl isatin)-based membrane (QP(SBP/BP)-20). The retention rates in hydroxide ion conductivity are 89.7 and 84.0% after soaking the membrane in 1 M KOH for 1152 h and in 4 M KOH for 628 h at 80 °C, respectively. The QP(SBP/BP)-20 membrane-based single-fuel cell exhibits an open-circuit voltage of 0.99 V and a peak power density of 744 mW cm–2 at 60 °C by fueling with humidified H2 and O2 with 0.05 MPa back pressure.

KeyWords AITranslate

fraction free volume spirobiindane microphase separation conductivity alkaline stability
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c00898

Chinese Library Classification Number:

Citation Information:

Designing the packing of polymer chains with reasonable fraction free volume (FFV) is regarded as an effective way to improve the conductivity of polymer-based membranes. We synthesize random polymers by copolymerization of bulky rigid-twisted spirobiindane, isatin, and one of the joint groups p-terphenyl, biphenyl, and 1,2-diphenylethane. The polycondensation reaction is catalyzed by trifluoromethanesulfonic acid. The introduced spirobiindane segments enlarge the distance of polymer chains and increase the FFV of the membrane. The formation of the microphase separation structure is evidenced according to the results of transmission electron microscopy and atomic force microscopy. As a result, a hydroxide conductivity of 126.7 mS cm–1 is achieved at 80 °C by the poly(spirobiindane diphenyl isatin)-based membrane (QP(SBP/BP)-20). The retention rates in hydroxide ion conductivity are 89.7 and 84.0% after soaking the membrane in 1 M KOH for 1152 h and in 4 M KOH for 628 h at 80 °C, respectively. The QP(SBP/BP)-20 membrane-based single-fuel cell exhibits an open-circuit voltage of 0.99 V and a peak power density of 744 mW cm–2 at 60 °C by fueling with humidified H2 and O2 with 0.05 MPa back pressure.

quote

GB/T 7714-2015 [1] Jinyan Chen, Shicheng Xu, Xin Su, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c00898.
MLA [1] Jinyan Chen, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c00898.
APA [1] Jinyan Chen, Shicheng Xu, Xin Su, Wei Wei, Yujiao Li, Ranli Du, & Ronghuan He. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c00898
IEEE [1] Jinyan Chen, Shicheng Xu, Xin Su, Wei Wei, Yujiao Li, Ranli Du, and Ronghuan He, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c00898. keywords: {fraction free volume;spirobiindane;microphase separation;conductivity;alkaline stability}