Disassembly of an Interconjugated Polyelectrolyte Complex Using Ionic Surfactants AITranslate

University of California; University of California; University of California
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The ability to manipulate the state of assembly of light-harvesting molecular materials can be important to control light-induced damage at high illumination intensities. Disassembly of such materials is thus an important consideration from a photoprotection perspective. Here, we show that an artificial light-harvesting antenna based on an interconjugated polyelectrolyte complex can be disassembled using ionic surfactants in aqueous solution. We demonstrate that both anionic and cationic surfactants can do so with comparable efficiency, thereby shutting electronic energy transfer between the exciton donor and acceptor conjugated polyelectrolytes. However, the structural evolution of the aqueous complexes both above and below the critical micelle concentration differed significantly depending on the sign of the ionic surfactant and the relative polyion charge ratio.

KeyWords AITranslate

Conjugated polyelectrolytes selfassembly ionic surfactants energy transfer small angle Xray scattering dynamic light scattering
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.9b00023

Chinese Library Classification Number:

Citation Information:

The ability to manipulate the state of assembly of light-harvesting molecular materials can be important to control light-induced damage at high illumination intensities. Disassembly of such materials is thus an important consideration from a photoprotection perspective. Here, we show that an artificial light-harvesting antenna based on an interconjugated polyelectrolyte complex can be disassembled using ionic surfactants in aqueous solution. We demonstrate that both anionic and cationic surfactants can do so with comparable efficiency, thereby shutting electronic energy transfer between the exciton donor and acceptor conjugated polyelectrolytes. However, the structural evolution of the aqueous complexes both above and below the critical micelle concentration differed significantly depending on the sign of the ionic surfactant and the relative polyion charge ratio.

quote

GB/T 7714-2015 [1] Carmen J. Segura, Marcos Lucero, Alexander L. Ayzner. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.9b00023.
MLA [1] Carmen J. Segura, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.9b00023.
APA [1] Carmen J. Segura, Marcos Lucero, & Alexander L. Ayzner. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.9b00023
IEEE [1] Carmen J. Segura, Marcos Lucero, and Alexander L. Ayzner, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.9b00023. keywords: {Conjugated polyelectrolytes;selfassembly;ionic surfactants;energy transfer;small angle Xray scattering;dynamic light scattering}