daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Development of metal-organic deposition-derived second-generation high-temperature superconductor tapes and artificial flux pinning AITranslate

Shanghai University; Shanghai University; Shanghai University; Shanghai University
AITranslate
Publisher: Springer Nature
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The second-generation high-temperature superconductor tape (2G-HTS, also known as a coated conductor) based on REBaCuO (REBa2Cu3O7–δ) exhibits high current density and potential cost-effective price/performance, compared with conventional superconducting materials. Using commercial 2G-HTS tapes, more than a dozen cable vendors had been manufacturing REBCO cables, such as the latest kilometer-class REBCO cable, which was incorporated into a civil grid on December 2021, as part of the record-breaking 35-kV-voltage superconductor cable demonstration project in downtown Shanghai. This paper describes the development of HTS-coated conductors, then outlines the various technological routes for their preparation, reviews the artificial flux pinning of coated conductors, and finally summarizes the technological breakthroughs, the latest research advances, and provides an outlook on their application prospects.

KeyWords AITranslate

Hightemperature superconductors RE123 superconductor tapes Chemical solution deposition Flux pinning
No data

Basic Information:

DOI:https://doi.org/10.1007/s40436-023-00447-z

Chinese Library Classification Number:

Citation Information:

The second-generation high-temperature superconductor tape (2G-HTS, also known as a coated conductor) based on REBaCuO (REBa2Cu3O7–δ) exhibits high current density and potential cost-effective price/performance, compared with conventional superconducting materials. Using commercial 2G-HTS tapes, more than a dozen cable vendors had been manufacturing REBCO cables, such as the latest kilometer-class REBCO cable, which was incorporated into a civil grid on December 2021, as part of the record-breaking 35-kV-voltage superconductor cable demonstration project in downtown Shanghai. This paper describes the development of HTS-coated conductors, then outlines the various technological routes for their preparation, reviews the artificial flux pinning of coated conductors, and finally summarizes the technological breakthroughs, the latest research advances, and provides an outlook on their application prospects.

quote

GB/T 7714-2015 [1] DongXu Wang, Jing Chen, DiFan Zhou, et al. Advances in Manufacturing, 2023(11). DOI:10.1007/s40436-023-00447-z.
MLA [1] DongXu Wang, et al., Advances in Manufacturing, no. 11, 2023, https://doi.org/10.1007/s40436-023-00447-z.
APA [1] DongXu Wang, Jing Chen, DiFan Zhou, & ChuanBing Cai. (2023). Advances in Manufacturing(11). https://doi.org/10.1007/s40436-023-00447-z
IEEE [1] DongXu Wang, Jing Chen, DiFan Zhou, and ChuanBing Cai, Advances in Manufacturing, no. 11, 2023, doi: 10.1007/s40436-023-00447-z. keywords: {Hightemperature superconductors;RE123 superconductor tapes;Chemical solution deposition;Flux pinning}