Tough, Healable, Photoresponsive Actuator Based on a Quadruple Hydrogen-Bond-Capped Slide-Ring Structure AITranslate
Abstract AITranslate
A tough self-healing supramolecular photoresponsive actuator based on a 2-urea-4[1H]-pyrimidinone (UPy)-terminated host–guest slide-ring structure was designed. The supramolecular gel was revealed to be stretchable and tough. It achieved a tensile strength of 2.25 MPa with elongation at break of 533% and could lift beyond 900 times its own weight. Based on the special structure, its photoresponsive motion was as fast as 55° within 40 s under 365 nm irradiation. The gel also showed highly efficient self-healable ability and quick responsivity to temperature and humidity.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.3c01683
Chinese Library Classification Number:
Citation Information:
A tough self-healing supramolecular photoresponsive actuator based on a 2-urea-4[1H]-pyrimidinone (UPy)-terminated host–guest slide-ring structure was designed. The supramolecular gel was revealed to be stretchable and tough. It achieved a tensile strength of 2.25 MPa with elongation at break of 533% and could lift beyond 900 times its own weight. Based on the special structure, its photoresponsive motion was as fast as 55° within 40 s under 365 nm irradiation. The gel also showed highly efficient self-healable ability and quick responsivity to temperature and humidity.
quote
| GB/T 7714-2015 | [1] Dandan Tian, Wenjing Ma, Lingji Zheng, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c01683. |
| MLA | [1] Dandan Tian, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c01683. |
| APA | [1] Dandan Tian, Wenjing Ma, Lingji Zheng, Kaixuan Jiang, Hu He, & Ruyi Sun. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c01683 |
| IEEE | [1] Dandan Tian, Wenjing Ma, Lingji Zheng, Kaixuan Jiang, Hu He, and Ruyi Sun, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c01683. keywords: {photoresponsive actuator;slidering structure;host−guest interaction;quadruple hydrogen bonds;healable hydrogel} |