daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Bidirectional Halide Ion Exchange in Paired Lead Halide Perovskite Films with Thermal Activation AITranslate

Technical University of Denmark; and Department of Chemical & Biomolecular Engineering University of Notre Dame; Technical University of Denmark; and Department of Chemical & Biomolecular Engineering University of Notre Dame
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

MAPbBr3 and MAPbI3 films cast onto glass slides and physically paired together undergo halide exchange to form mixed halide films. The change in halide composition in these two ∼130 nm thick films occurs concurrently with Br– diffusing toward the MAPbI3 film and I– diffusing toward the MAPbBr3 film. The diffusion of these halide species, which is tracked through changes in the absorption, offers a direct measurement of thermally activated halide diffusion in perovskite films. The increase in the rate constant of halide diffusion with increasing temperature (from 8.3 × 10–6 s–1 at 23 °C to 3.7 × 10–4 s–1 at 140 °C) follows an Arrhenius relationship with activation energy of 51 kJ/mol. The thermally activated halide exchange shows the challenges of employing layers of different metal halide perovskites in stable tandem solar cells.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.9b01280

Chinese Library Classification Number:

Citation Information:

MAPbBr3 and MAPbI3 films cast onto glass slides and physically paired together undergo halide exchange to form mixed halide films. The change in halide composition in these two ∼130 nm thick films occurs concurrently with Br– diffusing toward the MAPbI3 film and I– diffusing toward the MAPbBr3 film. The diffusion of these halide species, which is tracked through changes in the absorption, offers a direct measurement of thermally activated halide diffusion in perovskite films. The increase in the rate constant of halide diffusion with increasing temperature (from 8.3 × 10–6 s–1 at 23 °C to 3.7 × 10–4 s–1 at 140 °C) follows an Arrhenius relationship with activation energy of 51 kJ/mol. The thermally activated halide exchange shows the challenges of employing layers of different metal halide perovskites in stable tandem solar cells.

quote

GB/T 7714-2015 [1] Tor Elmelund, Rebecca A. Scheidt, Brian Seger, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.9b01280.
MLA [1] Tor Elmelund, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.9b01280.
APA [1] Tor Elmelund, Rebecca A. Scheidt, Brian Seger, & Prashant V. Kamat. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.9b01280
IEEE [1] Tor Elmelund, Rebecca A. Scheidt, Brian Seger, and Prashant V. Kamat, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.9b01280.