Inverted Pyramid Textured p-Silicon Covered with Co2P as an Efficient and Stable Solar Hydrogen Evolution Photocathode AITranslate
Abstract AITranslate
Silicon (Si) has been investigated as a promising photoelectrode material for use in photoelectrochemical water splitting. However, development of Si photocathodes that can operate at a high photocurrent density for solar-driven hydrogen production with long-term stability remains challenging. Herein, we report the fabrication of inverted pyramid textured p-Si photocathodes covered conformally and continuously with a thickness-gradient cobalt phosphide (Co2P) layer, which not only effectively isolates p-Si from aqueous electrolyte to avoid corrosion but also efficiently catalyzes the solar-driven hydrogen evolution reaction (HER). Thanks to the unique inverted pyramid structure, the drop-cast Co2P can distribute all over the p-Si photocathode and form a macroscopically continuous but locally nonuniform layer on the sidewalls of each inverted pyramid. The local nonuniform distribution enables light absorption to be partially separated from catalytic activity. Consequently, the as-fabricated Co2P-coated p-Si photocathode exhibits a high photocurrent density of 35.2 mA cm–2 at 0 V versus the reversible hydrogen electrode under AM 1.5G illumination and can photoelectrochemically catalyze the HER above 30 mA cm–2 at least 150 h without notable degradation.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.9b00964
Chinese Library Classification Number:
Citation Information:
Silicon (Si) has been investigated as a promising photoelectrode material for use in photoelectrochemical water splitting. However, development of Si photocathodes that can operate at a high photocurrent density for solar-driven hydrogen production with long-term stability remains challenging. Herein, we report the fabrication of inverted pyramid textured p-Si photocathodes covered conformally and continuously with a thickness-gradient cobalt phosphide (Co2P) layer, which not only effectively isolates p-Si from aqueous electrolyte to avoid corrosion but also efficiently catalyzes the solar-driven hydrogen evolution reaction (HER). Thanks to the unique inverted pyramid structure, the drop-cast Co2P can distribute all over the p-Si photocathode and form a macroscopically continuous but locally nonuniform layer on the sidewalls of each inverted pyramid. The local nonuniform distribution enables light absorption to be partially separated from catalytic activity. Consequently, the as-fabricated Co2P-coated p-Si photocathode exhibits a high photocurrent density of 35.2 mA cm–2 at 0 V versus the reversible hydrogen electrode under AM 1.5G illumination and can photoelectrochemically catalyze the HER above 30 mA cm–2 at least 150 h without notable degradation.
quote
| GB/T 7714-2015 | [1] Sitaramanjaneva Mouli Thalluri, Bin Wei, Katharina Welter, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.9b00964. |
| MLA | [1] Sitaramanjaneva Mouli Thalluri, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.9b00964. |
| APA | [1] Sitaramanjaneva Mouli Thalluri, Bin Wei, Katharina Welter, Rajesh Thomas, Vladimir Smirnov, Liang Qiao, Zhongchang Wang, Friedhelm Finger, & Lifeng Liu. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.9b00964 |
| IEEE | [1] Sitaramanjaneva Mouli Thalluri, Bin Wei, Katharina Welter, Rajesh Thomas, Vladimir Smirnov, Liang Qiao, Zhongchang Wang, Friedhelm Finger, and Lifeng Liu, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.9b00964. |