daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Low-Temperature and Solventless Ring-Opening Polymerization of Eutectic Mixtures of l-Lactide and Lactones for Biodegradable Polyesters AITranslate

University of Groningen; University of Groningen;Instituto de Ciencia de Materiales de Madrid (ICMM), Consejo Superior de Investigaciones Científicas (CSIC); Universidad Nacional Autónoma de México (UNAM);Centro de Investigación en Química Aplicada (CIQA); University of Groningen; Universidad Nacional Autónoma de México (UNAM)
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Biodegradability is one of the key features for reducing the negative environmental impact of plastic waste disposal; therefore, designing biocompatible polymeric biomaterials with programmable life cycles is urgently needed. Herein, deep eutectic solvent monomers (DESm) composed of l-lactide and various lactones of different molecular weights were formulated to obtain polyesters at low temperatures with the aid of organocatalysts and under solventless conditions. The introduced DESm expand the range of eutectic mixtures capable of undergoing ring-opening polymerization (ROP) to include mixtures of l-lactide with δ-valerolactone and δ-hexalactone. Extending the toolbox for DESm preparation will allow for the design of polyesters with tailored molecular weight and crystallinity, which are conducive to programmable degradability. ROP of DESm carried out at low temperatures and under solventless conditions holds promise for a sustainable framework for preparing biodegradable polymers for biomedical applications.

KeyWords AITranslate

ring opening polymerization deep eutectic solvent monomers: valerolactone lactide polyesters
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c00591

Chinese Library Classification Number:

Citation Information:

Biodegradability is one of the key features for reducing the negative environmental impact of plastic waste disposal; therefore, designing biocompatible polymeric biomaterials with programmable life cycles is urgently needed. Herein, deep eutectic solvent monomers (DESm) composed of l-lactide and various lactones of different molecular weights were formulated to obtain polyesters at low temperatures with the aid of organocatalysts and under solventless conditions. The introduced DESm expand the range of eutectic mixtures capable of undergoing ring-opening polymerization (ROP) to include mixtures of l-lactide with δ-valerolactone and δ-hexalactone. Extending the toolbox for DESm preparation will allow for the design of polyesters with tailored molecular weight and crystallinity, which are conducive to programmable degradability. ROP of DESm carried out at low temperatures and under solventless conditions holds promise for a sustainable framework for preparing biodegradable polymers for biomedical applications.

quote

GB/T 7714-2015 [1] Martín CastilloSantillan, Dina Maniar, María C. Gutiérrez, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c00591.
MLA [1] Martín CastilloSantillan, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c00591.
APA [1] Martín CastilloSantillan, Dina Maniar, María C. Gutiérrez, Priscila QuiñonezAngulo, José Román TorresLubian, Katja Loos, & Josué D. MotaMorales. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c00591
IEEE [1] Martín CastilloSantillan, Dina Maniar, María C. Gutiérrez, Priscila QuiñonezAngulo, José Román TorresLubian, Katja Loos, and Josué D. MotaMorales, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c00591. keywords: {ring opening polymerization;deep eutectic solvent monomers: valerolactone;lactide;polyesters}