Sulfonated Poly(arylene ether sulfone) Multi-Block Copolymers with Selectively Cross-Linked Domains for Proton Exchange Membranes AITranslate

University of Notre Dame; University of Notre Dame; University of Notre Dame; University of Notre Dame; University of Notre Dame; University of Notre Dame
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

A facile design of sulfonated poly(arylene ether sulfone) multi-block copolymer membranes with selectively cross-linked hydrophobic domains is reported for proton exchange membranes. The cross-linkable linear multi-block copolymers are prepared via coupling telechelic hydrophilic disulfonated oligomers (BPS100) and telechelic hydrophobic oligomers (PPA0) containing cross-linkable allyl-derivatized phenolphthalein moieties. The cross-linked membranes are prepared through UV-initiated thiol-ene cross-linking reactions between allyl-functionalized hydrophobic blocks with pentaerythritol tetrakis(3-mercaptopropionate) as a cross-linker. With highly cross-linked hydrophobic blocks and flexible hydrophilic blocks, the selectively cross-linked multiblock copolymer membranes exhibit remarkably improved dimensional stability and proton conductivity compared to the cross-linked random copolymers. The cross-linked membrane with the longest hydrophilic block length shows a remarkable proton conductivity of 123 mS/cm with a suppressed volume swelling ratio of 25% at 25 °C. At the highest ion exchange capacity level (2.25 meq/g) and the longest block length, the cross-linked multi-block copolymer membrane outperforms Nafion over the full relative humidity range.

KeyWords AITranslate

multiblock copolymers phenolphthalein selective crosslinking thiolene reaction proton exchange membrane
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c01204

Chinese Library Classification Number:

Citation Information:

A facile design of sulfonated poly(arylene ether sulfone) multi-block copolymer membranes with selectively cross-linked hydrophobic domains is reported for proton exchange membranes. The cross-linkable linear multi-block copolymers are prepared via coupling telechelic hydrophilic disulfonated oligomers (BPS100) and telechelic hydrophobic oligomers (PPA0) containing cross-linkable allyl-derivatized phenolphthalein moieties. The cross-linked membranes are prepared through UV-initiated thiol-ene cross-linking reactions between allyl-functionalized hydrophobic blocks with pentaerythritol tetrakis(3-mercaptopropionate) as a cross-linker. With highly cross-linked hydrophobic blocks and flexible hydrophilic blocks, the selectively cross-linked multiblock copolymer membranes exhibit remarkably improved dimensional stability and proton conductivity compared to the cross-linked random copolymers. The cross-linked membrane with the longest hydrophilic block length shows a remarkable proton conductivity of 123 mS/cm with a suppressed volume swelling ratio of 25% at 25 °C. At the highest ion exchange capacity level (2.25 meq/g) and the longest block length, the cross-linked multi-block copolymer membrane outperforms Nafion over the full relative humidity range.

quote

GB/T 7714-2015 [1] Tao Wang, Si Li, Tanner Corrado, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c01204.
MLA [1] Tao Wang, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c01204.
APA [1] Tao Wang, Si Li, Tanner Corrado, Lingyu Yang, Jennifer L. Schaefer, & Ruilan Guo. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c01204
IEEE [1] Tao Wang, Si Li, Tanner Corrado, Lingyu Yang, Jennifer L. Schaefer, and Ruilan Guo, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c01204. keywords: {multiblock copolymers;phenolphthalein;selective crosslinking;thiolene reaction;proton exchange membrane}