MXetronics: MXene-Enabled Electronic and Photonic Devices AITranslate

King Abdullah University of Science and Technology (KAUST); King Abdullah University of Science and Technology (KAUST)
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

MXenes are a rapidly growing family of two-dimensional (2D) materials based on transition-metal carbides and nitrides that have shown great potential as multifunctional nanomaterials. Their unique combination of metallic conductivity, hydrophilicity, and highly charged surfaces endow them with excellent electrochemical performance. Yes, these same characteristics are equally important in electronic and optoelectronic applications of MXenes, which are henceforth termed MXetronics. MXenes are suitable for solution processing in various polar solvents, allowing the preparation of MXene thin films with controlled transparency, sheet resistance, interlayer spacing, and surface chemistry. The wide selection of various MXene structures, transition-metal compositions, and surface functional groups enables tunable work function, band gap, and hence electronic and optical properties. In this Review, we summarize the recent advances in MXetronics and discuss future possibilities for this rising class of 2D materials.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsmaterialslett.9b00419

Chinese Library Classification Number:

Citation Information:

MXenes are a rapidly growing family of two-dimensional (2D) materials based on transition-metal carbides and nitrides that have shown great potential as multifunctional nanomaterials. Their unique combination of metallic conductivity, hydrophilicity, and highly charged surfaces endow them with excellent electrochemical performance. Yes, these same characteristics are equally important in electronic and optoelectronic applications of MXenes, which are henceforth termed MXetronics. MXenes are suitable for solution processing in various polar solvents, allowing the preparation of MXene thin films with controlled transparency, sheet resistance, interlayer spacing, and surface chemistry. The wide selection of various MXene structures, transition-metal compositions, and surface functional groups enables tunable work function, band gap, and hence electronic and optical properties. In this Review, we summarize the recent advances in MXetronics and discuss future possibilities for this rising class of 2D materials.

quote

GB/T 7714-2015 [1] Hyunho Kim, Husam N. Alshareef. ACS Materials Letters, 2020(2). DOI:10.1021/acsmaterialslett.9b00419.
MLA [1] Hyunho Kim, and Husam N. Alshareef. ACS Materials Letters, no. 2, 2020, https://doi.org/10.1021/acsmaterialslett.9b00419.
APA [1] Hyunho Kim, & Husam N. Alshareef. (2020). ACS Materials Letters(2). https://doi.org/10.1021/acsmaterialslett.9b00419
IEEE [1] Hyunho Kim and Husam N. Alshareef, ACS Materials Letters, no. 2, 2020, doi: 10.1021/acsmaterialslett.9b00419.