Unlocking the Potential of Polymeric Aerogels from Food and Agricultural Waste for Sustainable CO2 Capture AITranslate
Abstract AITranslate
The increase in waste generation from food processing and agricultural residues presents a significant challenge for sustainable development and waste management. Utilizing these biomass waste materials for valuable applications can help address this issue, while promoting a circular economy. In this context, the current study focuses on the valorization of waste materials of organic origin for CO2 capture, a crucial component in global efforts to mitigate climate change and reduce the planet’s warming. The investigated polymeric aerogels were synthesized using byproducts from food processing and agricultural residue waste products, specifically crustacean shells and sugarcane bagasse. A comprehensive set of analytical techniques, including viscometry, Fourier transform infrared spectroscopy (FTIR), energy dispersive X-ray spectroscopy (EDX), thermogravimetric analysis (TGA), X-ray diffraction (XRD), field emission scanning electron microscopy (FESEM), transmission electron microscopy (TEM), and Brunauer–Emmett–Teller (BET) surface area analysis, were employed to examine the physicochemical, thermal, microstructural, and textural properties of the prepared materials. These adsorbents demonstrated promising prospects for carbon dioxide capture, adsorbing up to 5.78 mg/g of the gas at 273 K and 2.82 mg/g at 298 K. Considering their sorption performance, the low cost of raw materials, and the potential for scaling up, this work further validates the adsorbent-based postcombustion carbon capture technology as an effective approach for addressing the detrimental consequences of carbon dioxide emissions.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.3c02269
Chinese Library Classification Number:
Citation Information:
The increase in waste generation from food processing and agricultural residues presents a significant challenge for sustainable development and waste management. Utilizing these biomass waste materials for valuable applications can help address this issue, while promoting a circular economy. In this context, the current study focuses on the valorization of waste materials of organic origin for CO2 capture, a crucial component in global efforts to mitigate climate change and reduce the planet’s warming. The investigated polymeric aerogels were synthesized using byproducts from food processing and agricultural residue waste products, specifically crustacean shells and sugarcane bagasse. A comprehensive set of analytical techniques, including viscometry, Fourier transform infrared spectroscopy (FTIR), energy dispersive X-ray spectroscopy (EDX), thermogravimetric analysis (TGA), X-ray diffraction (XRD), field emission scanning electron microscopy (FESEM), transmission electron microscopy (TEM), and Brunauer–Emmett–Teller (BET) surface area analysis, were employed to examine the physicochemical, thermal, microstructural, and textural properties of the prepared materials. These adsorbents demonstrated promising prospects for carbon dioxide capture, adsorbing up to 5.78 mg/g of the gas at 273 K and 2.82 mg/g at 298 K. Considering their sorption performance, the low cost of raw materials, and the potential for scaling up, this work further validates the adsorbent-based postcombustion carbon capture technology as an effective approach for addressing the detrimental consequences of carbon dioxide emissions.
quote
| GB/T 7714-2015 | [1] Victor James Oghenekohwo, Ahmed Abdelhamid Maamoun, Sonia Zulfiqar, et al. ACS Applied Polymer Materials, 2024(6). DOI:10.1021/acsapm.3c02269. |
| MLA | [1] Victor James Oghenekohwo, et al., ACS Applied Polymer Materials, no. 6, 2024, https://doi.org/10.1021/acsapm.3c02269. |
| APA | [1] Victor James Oghenekohwo, Ahmed Abdelhamid Maamoun, Sonia Zulfiqar, Michael J. Forrester, Václav Slovák, TungPing Wang, & Eric W. Cochran. (2024). ACS Applied Polymer Materials(6). https://doi.org/10.1021/acsapm.3c02269 |
| IEEE | [1] Victor James Oghenekohwo, Ahmed Abdelhamid Maamoun, Sonia Zulfiqar, Michael J. Forrester, Václav Slovák, TungPing Wang, and Eric W. Cochran, ACS Applied Polymer Materials, no. 6, 2024, doi: 10.1021/acsapm.3c02269. keywords: {chitosan;cellulose;sugarcane bagasse;aerogel;CO2 capture} |