daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Finely Interpenetrating Bulk Heterojunction Structure for Lead Sulfide Colloidal Quantum Dot Solar Cells by Convective Assembly AITranslate

Kyoto University; Kyoto University; Soochow University; Kyoto University; Soochow University; Soochow University; Kyoto University; Kyoto University; Kyoto University; Kyoto University; Soochow University; The University of Tokyo; Kyoto University; Soochow University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Lead chalcogenides colloidal quantum dot (PbS CQD) solar cells employing an ordered bulk heterojunction (OBHJ) structure allow sufficient utilization of solar energy and at the same time ensure efficient charge extractions. However, the interfacial deficiency was determined to be a significant limiting factor for the further improvement of efficiency. Herein, a finely interpenetrating OBHJ structure between zinc oxide nanowire (ZnO NW) arrays and PbS CQDs was achieved by simultaneously controlling the growth orientation of ZnO NWs and introducing convective assembly as the CQD deposition technique. The inherent directionality during the assembly process leads to dense packing and efficient infiltration of CQDs, forming a valid OBHJ structure. Additionally, a self-assembled monolayer was introduced to further improve the Voc deficit. As a result, a record PCE of 9.92% has been demonstrated for OBHJ structured CQD solar cells that are compatible with low-temperature and scalable manufacturing processes.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.9b00053

Chinese Library Classification Number:

Citation Information:

Lead chalcogenides colloidal quantum dot (PbS CQD) solar cells employing an ordered bulk heterojunction (OBHJ) structure allow sufficient utilization of solar energy and at the same time ensure efficient charge extractions. However, the interfacial deficiency was determined to be a significant limiting factor for the further improvement of efficiency. Herein, a finely interpenetrating OBHJ structure between zinc oxide nanowire (ZnO NW) arrays and PbS CQDs was achieved by simultaneously controlling the growth orientation of ZnO NWs and introducing convective assembly as the CQD deposition technique. The inherent directionality during the assembly process leads to dense packing and efficient infiltration of CQDs, forming a valid OBHJ structure. Additionally, a self-assembled monolayer was introduced to further improve the Voc deficit. As a result, a record PCE of 9.92% has been demonstrated for OBHJ structured CQD solar cells that are compatible with low-temperature and scalable manufacturing processes.

quote

GB/T 7714-2015 [1] Guozheng Shi, Anusit Kaewprajak, Xufeng Ling, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.9b00053.
MLA [1] Guozheng Shi, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.9b00053.
APA [1] Guozheng Shi, Anusit Kaewprajak, Xufeng Ling, Akinobu Hayakawa, Sijie Zhou, Bin Song, YangWon Kang, Takahiro Hayashi, Mutlu Ege Altun, Masahiro Nakaya, Zeke Liu, Haibin Wang, Takashi Sagawa, & Wanli Ma. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.9b00053
IEEE [1] Guozheng Shi, Anusit Kaewprajak, Xufeng Ling, Akinobu Hayakawa, Sijie Zhou, Bin Song, YangWon Kang, Takahiro Hayashi, Mutlu Ege Altun, Masahiro Nakaya, Zeke Liu, Haibin Wang, Takashi Sagawa, and Wanli Ma, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.9b00053.