Biobased Multifunctional Poly(lactic acid) Nanofiber Membranes for Efficient Personal Thermal Management AITranslate

Qingdao University; Shaoxing University; Qingdao University; Qingdao University; Qingdao University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The growing demand for efficient and economical cooling in both indoor and outdoor applications, especially personal cooling in outdoor environments, is a major challenge globally today. Passive daytime radiative cooling technology with spectral selectivity which operates by transferring radiative heat into cold universe (∼3 K) through the atmospheric window (8–13 μm) is an emerging and sustainable cooling technology. However, passive daytime radiative cooling materials are still limited by nondegradable, finite categories and single function. In this paper, multifunctional biobased poly(lactic acid) (PLA)/poly(butylene succinate) (PBS) nanofiber membranes with radiation cooling, electrical conductivity, and antibacterial properties were prepared by electrospinning technology combined with spraying technology. This multifunctional nanofiber membrane has high solar reflectivity (82%) and strong mid-infrared emissivity (98%) that achieves a temperature drop of 5.5–12 °C on sunny days and 2.9–10 °C on cloudy days. Adding 18.2% silver nanowires can reduce the resistance of the nanofiber membrane to 208 Ω, which also endowed the membrane with good antibacterial properties. This multifunctional nanofiber membrane opens up an environmentally sustainable approach for personal thermal management and introduces new possibilities for the rational design of next-generation smart textiles.

KeyWords AITranslate

Biocompatibility Personal thermal management Passive daytime radiative cooling Hierarchically porous fiber Electrospinning
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c02516

Chinese Library Classification Number:

Citation Information:

The growing demand for efficient and economical cooling in both indoor and outdoor applications, especially personal cooling in outdoor environments, is a major challenge globally today. Passive daytime radiative cooling technology with spectral selectivity which operates by transferring radiative heat into cold universe (∼3 K) through the atmospheric window (8–13 μm) is an emerging and sustainable cooling technology. However, passive daytime radiative cooling materials are still limited by nondegradable, finite categories and single function. In this paper, multifunctional biobased poly(lactic acid) (PLA)/poly(butylene succinate) (PBS) nanofiber membranes with radiation cooling, electrical conductivity, and antibacterial properties were prepared by electrospinning technology combined with spraying technology. This multifunctional nanofiber membrane has high solar reflectivity (82%) and strong mid-infrared emissivity (98%) that achieves a temperature drop of 5.5–12 °C on sunny days and 2.9–10 °C on cloudy days. Adding 18.2% silver nanowires can reduce the resistance of the nanofiber membrane to 208 Ω, which also endowed the membrane with good antibacterial properties. This multifunctional nanofiber membrane opens up an environmentally sustainable approach for personal thermal management and introduces new possibilities for the rational design of next-generation smart textiles.

quote

GB/T 7714-2015 [1] Kaiqi Zhang, Shenglong Shang, Yu Zheng, et al. ACS Applied Polymer Materials, 2024(6). DOI:10.1021/acsapm.3c02516.
MLA [1] Kaiqi Zhang, et al., ACS Applied Polymer Materials, no. 6, 2024, https://doi.org/10.1021/acsapm.3c02516.
APA [1] Kaiqi Zhang, Shenglong Shang, Yu Zheng, Luyao Wei, & Ping Zhu. (2024). ACS Applied Polymer Materials(6). https://doi.org/10.1021/acsapm.3c02516
IEEE [1] Kaiqi Zhang, Shenglong Shang, Yu Zheng, Luyao Wei, and Ping Zhu, ACS Applied Polymer Materials, no. 6, 2024, doi: 10.1021/acsapm.3c02516. keywords: {Biocompatibility;Personal thermal management;Passive daytime radiative cooling;Hierarchically porous fiber;Electrospinning}