daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Dewetting Effects in Poly(vinylidene fluoride-trifluoroethylene) Thin Films on Poly(3-hexylthiophene) Substrates AITranslate

Instituto de Estructura de la Materia;Instituto de Química Física Blas Cabrera;Instituto de Estructura de la Materia;Instituto de Estructura de la Materia
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Bilayers of ferroelectric polymers [poly(vinylidene fluoride-trifluoroethylene), PVDF-TrFE] on semiconducting poly(3-hexylthiophene) (P3HT) substrates have been prepared by sequential spin coating. When creating thin layers of PVDF-TrFE from its solution in methyl ether ketone (MEK), they exhibit dewetting in the form of holes for thicker P3HT substrates, whereas they form continuous layers on thinner P3HT substrates. The dispersive and polar components of the surface tension of the different P3HT substrates were obtained through contact angle measurements. An estimation of the shape of the disjoining pressure as a function of thickness of a liquid film of MEK on top of the different P3HT substrates was obtained. Through these estimations, we observe that the stability region for continuous film formation shifts toward higher thicknesses for the samples where experimentally the holes are observed. This work provides understanding on the mechanism of stable film formation and effective tools to control the formation of holes, in functional polymer bilayers, of special importance in the fabrication of organic thin film-based devices.

KeyWords AITranslate

dewetting spin coating piezoresponse force microscopy conductive atomic force microscopy surface tension spin coating
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c01234

Chinese Library Classification Number:

Citation Information:

Bilayers of ferroelectric polymers [poly(vinylidene fluoride-trifluoroethylene), PVDF-TrFE] on semiconducting poly(3-hexylthiophene) (P3HT) substrates have been prepared by sequential spin coating. When creating thin layers of PVDF-TrFE from its solution in methyl ether ketone (MEK), they exhibit dewetting in the form of holes for thicker P3HT substrates, whereas they form continuous layers on thinner P3HT substrates. The dispersive and polar components of the surface tension of the different P3HT substrates were obtained through contact angle measurements. An estimation of the shape of the disjoining pressure as a function of thickness of a liquid film of MEK on top of the different P3HT substrates was obtained. Through these estimations, we observe that the stability region for continuous film formation shifts toward higher thicknesses for the samples where experimentally the holes are observed. This work provides understanding on the mechanism of stable film formation and effective tools to control the formation of holes, in functional polymer bilayers, of special importance in the fabrication of organic thin film-based devices.

quote

GB/T 7714-2015 [1] Jing Cui, Esther Rebollar, Tiberio Ezquerra, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c01234.
MLA [1] Jing Cui, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c01234.
APA [1] Jing Cui, Esther Rebollar, Tiberio Ezquerra, & Aurora Nogales. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c01234
IEEE [1] Jing Cui, Esther Rebollar, Tiberio Ezquerra, and Aurora Nogales, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c01234. keywords: {dewetting;spin coating;piezoresponse force microscopy;conductive atomic force microscopy;surface tension;spin coating}