Nickel Isonicotinate Framework with Optimal Pore Structure for Complete Discrimination of Hexane Isomers AITranslate

Rutgers University;Hoffmann Institute of Advanced Materials; Wake Forest University; University of North Texas; University of North Texas; Wake Forest University;Hoffmann Institute of Advanced Materials; Rutgers University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Efficient separation of physicochemically similar alkanes is of vital importance. Adsorptive separation utilizing porous materials such as metal–organic frameworks with tunable pore structure and surface functionality represents an energy-efficient technology. In this study, we demonstrate successful separation of alkanes with varying degree of branching using a microporous nickel isonicotinate framework, Ni(4-PyC)2. Its 2-fold interpenetrated diamondoid structure with well-suited pore size enables selective adsorption of linear and monobranched hexane isomers, while excluding dibranched isomer. Breakthrough experiments validated its capability to completely discriminate all three hexane isomers. Ab initio calculations combined with in situ infrared spectroscopic analysis unveiled the nature of host–guest interactions and differences in the binding energies and diffusion barriers among the isomers. Having well-balanced adsorption uptakes (146 and 79 mg g–1 of nHEX and 3MP), high nHEX/DMB uptake ratio (12.2) and fast kinetics, Ni(4-PyC)2 stands out as a promising adsorbent for complete separation of hexane isomers under ambient conditions.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsmaterialslett.3c01278

Chinese Library Classification Number:

Citation Information:

Efficient separation of physicochemically similar alkanes is of vital importance. Adsorptive separation utilizing porous materials such as metal–organic frameworks with tunable pore structure and surface functionality represents an energy-efficient technology. In this study, we demonstrate successful separation of alkanes with varying degree of branching using a microporous nickel isonicotinate framework, Ni(4-PyC)2. Its 2-fold interpenetrated diamondoid structure with well-suited pore size enables selective adsorption of linear and monobranched hexane isomers, while excluding dibranched isomer. Breakthrough experiments validated its capability to completely discriminate all three hexane isomers. Ab initio calculations combined with in situ infrared spectroscopic analysis unveiled the nature of host–guest interactions and differences in the binding energies and diffusion barriers among the isomers. Having well-balanced adsorption uptakes (146 and 79 mg g–1 of nHEX and 3MP), high nHEX/DMB uptake ratio (12.2) and fast kinetics, Ni(4-PyC)2 stands out as a promising adsorbent for complete separation of hexane isomers under ambient conditions.

quote

GB/T 7714-2015 [1] Feng Xie, Liang Yu, Trevor Jenkins, et al. ACS Materials Letters, 2024(6). DOI:10.1021/acsmaterialslett.3c01278.
MLA [1] Feng Xie, et al., ACS Materials Letters, no. 6, 2024, https://doi.org/10.1021/acsmaterialslett.3c01278.
APA [1] Feng Xie, Liang Yu, Trevor Jenkins, Jocelyn Shutak, Kui Tan, Timo Thonhauser, Hao Wang, & Jing Li. (2024). ACS Materials Letters(6). https://doi.org/10.1021/acsmaterialslett.3c01278
IEEE [1] Feng Xie, Liang Yu, Trevor Jenkins, Jocelyn Shutak, Kui Tan, Timo Thonhauser, Hao Wang, and Jing Li, ACS Materials Letters, no. 6, 2024, doi: 10.1021/acsmaterialslett.3c01278.