daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Mechanistic Insight into the Precursor Chemistry of Cesium Tin Iodide Perovskite Nanocrystals AITranslate

Hokkaido University; Hokkaido University; Hokkaido University; Chuo University; National Institute for Materials Science (NIMS)
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Colloidal tin halide perovskite nanocrystals (NCs) are of interest as an alternative to their lead-based counterparts. While some advancements have been achieved in their synthetic development, the reaction mechanism, especially the precursor chemistry, of tin halide perovskite NCs remains poorly understood. Here, using cesium tin iodide (CsSnI3) perovskite NCs as a model system, we report on the mechanistic insight into the precursor chemistry of tin-based perovskite NCs through a combination of infrared, mass spectrometry, and nuclear magnetic resonance spectroscopy. We identify that the active intermediate complexes, polymeric alkanoate iodides that form via the reaction of the iodide source with oligomers present in the tin(II) carboxylates, play a key role in governing the reactivity of the tin iodide precursor, which leads to the variation in the size, size uniformity, and photoluminescence quantum yield of CsSnI3 NCs. Our work underscores the importance of understanding the precursor chemistry as a key parameter to design and synthesize tin halide perovskite NCs, which not only aids in their syntheses by design but also might benefit the fabrication of high-quality polycrystalline tin-based films.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsmaterialslett.3c00413

Chinese Library Classification Number:

Citation Information:

Colloidal tin halide perovskite nanocrystals (NCs) are of interest as an alternative to their lead-based counterparts. While some advancements have been achieved in their synthetic development, the reaction mechanism, especially the precursor chemistry, of tin halide perovskite NCs remains poorly understood. Here, using cesium tin iodide (CsSnI3) perovskite NCs as a model system, we report on the mechanistic insight into the precursor chemistry of tin-based perovskite NCs through a combination of infrared, mass spectrometry, and nuclear magnetic resonance spectroscopy. We identify that the active intermediate complexes, polymeric alkanoate iodides that form via the reaction of the iodide source with oligomers present in the tin(II) carboxylates, play a key role in governing the reactivity of the tin iodide precursor, which leads to the variation in the size, size uniformity, and photoluminescence quantum yield of CsSnI3 NCs. Our work underscores the importance of understanding the precursor chemistry as a key parameter to design and synthesize tin halide perovskite NCs, which not only aids in their syntheses by design but also might benefit the fabrication of high-quality polycrystalline tin-based films.

quote

GB/T 7714-2015 [1] BinBin Zhang, JiaKai Chen, Cong Zhang, et al. ACS Materials Letters, 2023(5). DOI:10.1021/acsmaterialslett.3c00413.
MLA [1] BinBin Zhang, et al., ACS Materials Letters, no. 5, 2023, https://doi.org/10.1021/acsmaterialslett.3c00413.
APA [1] BinBin Zhang, JiaKai Chen, Cong Zhang, Naoto Shirahata, & HongTao Sun. (2023). ACS Materials Letters(5). https://doi.org/10.1021/acsmaterialslett.3c00413
IEEE [1] BinBin Zhang, JiaKai Chen, Cong Zhang, Naoto Shirahata, and HongTao Sun, ACS Materials Letters, no. 5, 2023, doi: 10.1021/acsmaterialslett.3c00413.