daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Highly Stretchable and Reversibly Photomodulated PEDOT:PSS/PVA Films AITranslate

National Yang Ming Chiao Tung University; National Yang Ming Chiao Tung University; National Yang Ming Chiao Tung University; National Yang Ming Chiao Tung University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

This study presents highly stretchable and photomodulated poly(3,4-ethylenedioxythiophene) polystyrene sulfonate (PEDOT:PSS)/poly(vinyl alcohol) (PVA) composite films with improved mechanical strength and controllable conductivity. By incorporating water-soluble PVA and physically cross-linking PEDOT:PSS and PVA using acetone as bad solvent for the polymers, the films achieve a maximum strain of nearly 770%. The addition of spiropyran as a secondary dopant enables the reversible control of PEDOT:PSS conductivity through photochromic properties. The findings highlight the potential of these composite films for various applications, offering stretchability and tunable conductivity.

KeyWords AITranslate

conjugated polymer PEDOT:PSS photomodulated conductivity stretchability UV responsiveness
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c00808

Chinese Library Classification Number:

Citation Information:

This study presents highly stretchable and photomodulated poly(3,4-ethylenedioxythiophene) polystyrene sulfonate (PEDOT:PSS)/poly(vinyl alcohol) (PVA) composite films with improved mechanical strength and controllable conductivity. By incorporating water-soluble PVA and physically cross-linking PEDOT:PSS and PVA using acetone as bad solvent for the polymers, the films achieve a maximum strain of nearly 770%. The addition of spiropyran as a secondary dopant enables the reversible control of PEDOT:PSS conductivity through photochromic properties. The findings highlight the potential of these composite films for various applications, offering stretchability and tunable conductivity.

quote

GB/T 7714-2015 [1] HuanWei Lin, ChiaWei Chang, HsunHao Hsu, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c00808.
MLA [1] HuanWei Lin, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c00808.
APA [1] HuanWei Lin, ChiaWei Chang, HsunHao Hsu, & JiunTai Chen. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c00808
IEEE [1] HuanWei Lin, ChiaWei Chang, HsunHao Hsu, and JiunTai Chen, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c00808. keywords: {conjugated polymer;PEDOT:PSS;photomodulated conductivity;stretchability;UV responsiveness}