daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Advanced Acrylate Dielectric Elastomers with Large Actuation Strains at Very Low Electric Field AITranslate

Zheng Zhou University; Zheng Zhou University; Zheng Zhou University; Zheng Zhou University; Tsinghua University; Tsinghua University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Dielectric elastomers (DEs) are widely studied as artificial muscles due to their large actuation strain and fast electromechanical response. Currently, the commonly used acrylate DEs require high prestretching and are subjected to a high actuation electric field to achieve excellent actuation performance. In this work, we prepared DEs with very simple prescriptions by UV curing method. The prepared DEs have very low mechanical losses (<4%) and high dielectric constants (≥5.67) and obtain a large actuation strain (30.2%) under a relatively low electric field (31.6 kV/mm) with non-prestretching. This is because the soft butyl acrylate (BA) can guarantee the DEs with low Young‘s modulus and increase the dielectric constant by its polar functional group (-COO-), besides controlling the content of the cross-linker urethane acrylate (TR-U201XS) to regulate the cross-link density of the DEs and further influence its electromechanical properties, which are positive for improving the DEs’ actuation performance. And the DEs can be used to fabricate a fishtail-type device, which obtains a large swing range of about 90° in air and can overcome the resistance of water to work in water.

KeyWords AITranslate

dielectric elastomers crosslink density nonprestretching actuation performance fishtailtype device
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c01293

Chinese Library Classification Number:

Citation Information:

Dielectric elastomers (DEs) are widely studied as artificial muscles due to their large actuation strain and fast electromechanical response. Currently, the commonly used acrylate DEs require high prestretching and are subjected to a high actuation electric field to achieve excellent actuation performance. In this work, we prepared DEs with very simple prescriptions by UV curing method. The prepared DEs have very low mechanical losses (<4%) and high dielectric constants (≥5.67) and obtain a large actuation strain (30.2%) under a relatively low electric field (31.6 kV/mm) with non-prestretching. This is because the soft butyl acrylate (BA) can guarantee the DEs with low Young‘s modulus and increase the dielectric constant by its polar functional group (-COO-), besides controlling the content of the cross-linker urethane acrylate (TR-U201XS) to regulate the cross-link density of the DEs and further influence its electromechanical properties, which are positive for improving the DEs’ actuation performance. And the DEs can be used to fabricate a fishtail-type device, which obtains a large swing range of about 90° in air and can overcome the resistance of water to work in water.

quote

GB/T 7714-2015 [1] Yu Zhao, QiYao Feng, YaKun Xie, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c01293.
MLA [1] Yu Zhao, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c01293.
APA [1] Yu Zhao, QiYao Feng, YaKun Xie, ZiLi Zhang, LiJuan Yin, & ZhiMin Dang. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c01293
IEEE [1] Yu Zhao, QiYao Feng, YaKun Xie, ZiLi Zhang, LiJuan Yin, and ZhiMin Dang, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c01293. keywords: {dielectric elastomers;crosslink density;nonprestretching;actuation performance;fishtailtype device}