A Cost-Effective Semiconducting Polymer with an Ether Chain-Substituted Bithiophene as the Donor Unit Enabling Effective NIR-II Photoacoustic Imaging AITranslate
Abstract AITranslate
Due to their tunability in the chemical structure and light absorption, semiconducting polymers (SPs) have proven their promising potential for photoacoustic (PA) imaging within the second near-infrared (NIR-II) window. However, the syntheses of these polymers are generally lengthy and costly, limiting their potential applications. Herein, inspired by the commonly cost-effective thiophene-based compounds, we report a semiconducting polymer PTT-ATQ based on the non-fused ether chain-substituted donor unit 3,3′-bis(2-(2-(2-methoxyethoxy)ethoxy)ethoxy)-2,2′-bithiophene (TT). With the side chain substituted by the biocompatible ether chains, the TT unit possesses an even stronger electron-donating ability and thus, a strong intramolecular charge-transfer (ICT) effect in the polymer backbone; hence, an absorption band (peaked at ca. 1370 nm) within the NIR-II window for PTT-ATQ is realized. Meanwhile, the long and bulky side chains of the donor and acceptor units lead to a non-coplanarity in the polymer backbone, resulting in a twisted ICT effect that can induce high PA signals. Further results show that the PTT-ATQ has good biocompatibility and high in vivo PA imaging performance within the NIR-II window. This work highlights the effective strategy to realize high-performance NIR-II in vivo PA imaging SP contrast agents by using the cost-effective thiophene-based building blocks.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.3c00098
Chinese Library Classification Number:
Citation Information:
Due to their tunability in the chemical structure and light absorption, semiconducting polymers (SPs) have proven their promising potential for photoacoustic (PA) imaging within the second near-infrared (NIR-II) window. However, the syntheses of these polymers are generally lengthy and costly, limiting their potential applications. Herein, inspired by the commonly cost-effective thiophene-based compounds, we report a semiconducting polymer PTT-ATQ based on the non-fused ether chain-substituted donor unit 3,3′-bis(2-(2-(2-methoxyethoxy)ethoxy)ethoxy)-2,2′-bithiophene (TT). With the side chain substituted by the biocompatible ether chains, the TT unit possesses an even stronger electron-donating ability and thus, a strong intramolecular charge-transfer (ICT) effect in the polymer backbone; hence, an absorption band (peaked at ca. 1370 nm) within the NIR-II window for PTT-ATQ is realized. Meanwhile, the long and bulky side chains of the donor and acceptor units lead to a non-coplanarity in the polymer backbone, resulting in a twisted ICT effect that can induce high PA signals. Further results show that the PTT-ATQ has good biocompatibility and high in vivo PA imaging performance within the NIR-II window. This work highlights the effective strategy to realize high-performance NIR-II in vivo PA imaging SP contrast agents by using the cost-effective thiophene-based building blocks.
quote
| GB/T 7714-2015 | [1] Fan Jiang, Yintao Lan, Tiantian Zhou, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c00098. |
| MLA | [1] Fan Jiang, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c00098. |
| APA | [1] Fan Jiang, Yintao Lan, Tiantian Zhou, Jinya Hu, Yanfeng Zhang, Qian Li, Haijian Zhong, Pengfei Wei, Jian Zhang, Xuelong Huang, & Zhixiong Cao. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c00098 |
| IEEE | [1] Fan Jiang, Yintao Lan, Tiantian Zhou, Jinya Hu, Yanfeng Zhang, Qian Li, Haijian Zhong, Pengfei Wei, Jian Zhang, Xuelong Huang, and Zhixiong Cao, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c00098. keywords: {photoacoustic imaging (PAI);second near infrared (NIRII) window;costeffective;semiconducting polymer;nonfused ether;Show More} |