Early Stage Li Plating by Liquid Phase and Cryogenic Transmission Electron Microscopy AITranslate
Abstract AITranslate
Li metal anodes are among the most promising options for next-generation batteries, exhibiting the highest theoretical capacity. However, irregular Li electrodeposition, which raises safety concerns, is a major obstacle in practical applications. Therefore, a fundamental understanding of the beginning phases of Li plating, such as nucleation and early growth, which have a decisive influence on the dendritic growth of Li, is essential. In this study, we investigated the early stage of Li plating at the single-particle level and its correlation with the solid-electrolyte interphase (SEI) using in situ liquid phase transmission electron microscopy (TEM) and cryogenic TEM. We observed contrasting nucleation dynamics and particle growth patterns in two electrolytes (1 M LiPF6 in ethylene carbonate/diethyl carbonate and 1 M LiTFSI in 1,3-dioxolane/dimethoxy ethane), which originate from different chemical and physical properties of the SEIs. Based on our findings, we propose a mechanism of nucleation and initial growth of Li dictated by the SEI.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.2c02387
Chinese Library Classification Number:
Citation Information:
Li metal anodes are among the most promising options for next-generation batteries, exhibiting the highest theoretical capacity. However, irregular Li electrodeposition, which raises safety concerns, is a major obstacle in practical applications. Therefore, a fundamental understanding of the beginning phases of Li plating, such as nucleation and early growth, which have a decisive influence on the dendritic growth of Li, is essential. In this study, we investigated the early stage of Li plating at the single-particle level and its correlation with the solid-electrolyte interphase (SEI) using in situ liquid phase transmission electron microscopy (TEM) and cryogenic TEM. We observed contrasting nucleation dynamics and particle growth patterns in two electrolytes (1 M LiPF6 in ethylene carbonate/diethyl carbonate and 1 M LiTFSI in 1,3-dioxolane/dimethoxy ethane), which originate from different chemical and physical properties of the SEIs. Based on our findings, we propose a mechanism of nucleation and initial growth of Li dictated by the SEI.
quote
| GB/T 7714-2015 | [1] Hayoung Park, Yonggoon Jeon, Woo Jun Chung, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.2c02387. |
| MLA | [1] Hayoung Park, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.2c02387. |
| APA | [1] Hayoung Park, Yonggoon Jeon, Woo Jun Chung, Yuna Bae, Jihoon Kim, Hayeon Baek, & Jungwon Park. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.2c02387 |
| IEEE | [1] Hayoung Park, Yonggoon Jeon, Woo Jun Chung, Yuna Bae, Jihoon Kim, Hayeon Baek, and Jungwon Park, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.2c02387. |