daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Acrylate-Modified Aqueous Polyurethane Based on Oxime–Carbamate Structure with Transparent, Healable, and Fluorescent Properties AITranslate

Changchun University of Science and Technology; Changchun University of Science and Technology; Changchun University of Science and Technology; Changchun University of Science and Technology; Changchun University of Science and Technology; Changchun University of Science and Technology; Changchun University of Science and Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Acrylate-modified aqueous polyurethane has become a widely used material due to its good physical and versatile chemical properties. However, owing to damage resulting from daily use, which often limits polymer performance, it is important to prepare a transparent and repairable polyurethane material. In this work, an acrylate-modified aqueous polyurethane based on the reversible structure of oxime–carbamate of butanedione oxime (POU) was prepared. The visible-light transmittance of the POU film could exceed 70%; its tensile strength and elongation at break could reach 3.0 MPa and 493%, respectively, and the POU film had a tensile strength of 3.9 MPa and elongation at break of 589% after repair. In addition, the POU has adjustable fluorescence properties, which makes this material suitable for potential application in the field of information encryption.

KeyWords AITranslate

Polyurethane acrylate Film Healing Fluorescence Oxime−carbamate bonds
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c00485

Chinese Library Classification Number:

Citation Information:

Acrylate-modified aqueous polyurethane has become a widely used material due to its good physical and versatile chemical properties. However, owing to damage resulting from daily use, which often limits polymer performance, it is important to prepare a transparent and repairable polyurethane material. In this work, an acrylate-modified aqueous polyurethane based on the reversible structure of oxime–carbamate of butanedione oxime (POU) was prepared. The visible-light transmittance of the POU film could exceed 70%; its tensile strength and elongation at break could reach 3.0 MPa and 493%, respectively, and the POU film had a tensile strength of 3.9 MPa and elongation at break of 589% after repair. In addition, the POU has adjustable fluorescence properties, which makes this material suitable for potential application in the field of information encryption.

quote

GB/T 7714-2015 [1] Xu Pan, Wei Bai, Jinfang Liu, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c00485.
MLA [1] Xu Pan, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c00485.
APA [1] Xu Pan, Wei Bai, Jinfang Liu, Wenfu Zhang, Xuefeng Sheng, Yang Zhou, & Jianfu Zhang. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c00485
IEEE [1] Xu Pan, Wei Bai, Jinfang Liu, Wenfu Zhang, Xuefeng Sheng, Yang Zhou, and Jianfu Zhang, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c00485. keywords: {Polyurethane acrylate;Film;Healing;Fluorescence;Oxime−carbamate bonds}