How Stable Is the 2D/3D Interface of Metal Halide Perovskite under Light and Heat? AITranslate

University of Notre Dame; University of Notre Dame; University of Notre Dame
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

A (PEA)2PbI4 (2D) layer deposited on a MAPbI3 (3D) film undergoes a transformation upon photoirradiation and thermal treatment. The decrease in absorption and emission of the 2D layer during light and heat exposure, which shows migration of the PEA+ cation within the 3D film, points out the dynamic nature of the 2D/3D interface and intermixing of the two phases.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.2c02408

Chinese Library Classification Number:

Citation Information:

A (PEA)2PbI4 (2D) layer deposited on a MAPbI3 (3D) film undergoes a transformation upon photoirradiation and thermal treatment. The decrease in absorption and emission of the 2D layer during light and heat exposure, which shows migration of the PEA+ cation within the 3D film, points out the dynamic nature of the 2D/3D interface and intermixing of the two phases.

quote

GB/T 7714-2015 [1] Jishnudas Chakkamalayath, Nathaniel Hiott, Prashant V. Kamat. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.2c02408.
MLA [1] Jishnudas Chakkamalayath, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.2c02408.
APA [1] Jishnudas Chakkamalayath, Nathaniel Hiott, & Prashant V. Kamat. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.2c02408
IEEE [1] Jishnudas Chakkamalayath, Nathaniel Hiott, and Prashant V. Kamat, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.2c02408.