daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Fabrication of Recyclable Polyurethane Elastomers with Excellent Mechanical and Creep-Resistant Properties Based on a Bio-Sourced Azine Chain Extender AITranslate

Jiangnan University; Jiangnan University; Jiangnan University; Jiangnan University; Jiangnan University; Jiangnan University; Jiangnan University; Jiangnan University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Dynamic covalent polymers (DCPs) have attracted extensive attention as they integrate the advantages of thermoset and thermoplastic resins. However, the heat resistance was compromised due to the unstable features of dynamic covalent bonds. Therefore, it is still a challenge to develop DCPs possessing excellent heat resistance and recycling properties at the same time. Moreover, production and employment of biomass-derived chemicals have become increasingly urgent due to the petroleum shortage and environmental problems. Herein, a biomass-sourced azine chain extender was synthesized from biomass platform compound, 5-hydroxymethylfurfural. Small-molecule model furan azine compounds were synthesized to investigate the exchange mechanism at a high temperature. A series of azine polyurethane elastomers were prepared, containing different ratios of furan azine chain extenders. The synthesized furan azine polyurethane elastomers (FAPUEs-3) exhibited excellent mechanical properties compared with the control sample (FAPUEs-3CS), probably owing to the rigidity and polarity of furan rings. The obtained FAPUEs also showed excellent creep resistance at high temperatures by virtue of high exchange temperatures of furan azine moieties. The FAPUEs can be easily degraded under acidic conditions in acetone. The recovery rate of tensile strength could be still above 90% after 3 recycles at 150 °C under a pressure of 10 MPa. FAPUEs also showed excellent antibacterial effects against E. coli and S. aureus as azine moieties are a special kind of Schiff base. The FAPUEs opened an avenue for developing biomass-sourced recyclable PUEs.

KeyWords AITranslate

biosourced azine dynamic crosslinking networks polyurethane elastomers creep resistance reprocessability
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c02336

Chinese Library Classification Number:

Citation Information:

Dynamic covalent polymers (DCPs) have attracted extensive attention as they integrate the advantages of thermoset and thermoplastic resins. However, the heat resistance was compromised due to the unstable features of dynamic covalent bonds. Therefore, it is still a challenge to develop DCPs possessing excellent heat resistance and recycling properties at the same time. Moreover, production and employment of biomass-derived chemicals have become increasingly urgent due to the petroleum shortage and environmental problems. Herein, a biomass-sourced azine chain extender was synthesized from biomass platform compound, 5-hydroxymethylfurfural. Small-molecule model furan azine compounds were synthesized to investigate the exchange mechanism at a high temperature. A series of azine polyurethane elastomers were prepared, containing different ratios of furan azine chain extenders. The synthesized furan azine polyurethane elastomers (FAPUEs-3) exhibited excellent mechanical properties compared with the control sample (FAPUEs-3CS), probably owing to the rigidity and polarity of furan rings. The obtained FAPUEs also showed excellent creep resistance at high temperatures by virtue of high exchange temperatures of furan azine moieties. The FAPUEs can be easily degraded under acidic conditions in acetone. The recovery rate of tensile strength could be still above 90% after 3 recycles at 150 °C under a pressure of 10 MPa. FAPUEs also showed excellent antibacterial effects against E. coli and S. aureus as azine moieties are a special kind of Schiff base. The FAPUEs opened an avenue for developing biomass-sourced recyclable PUEs.

quote

GB/T 7714-2015 [1] Jinshi Han, Siyuan Li, Wei Zhang, et al. ACS Applied Polymer Materials, 2024(6). DOI:10.1021/acsapm.3c02336.
MLA [1] Jinshi Han, et al., ACS Applied Polymer Materials, no. 6, 2024, https://doi.org/10.1021/acsapm.3c02336.
APA [1] Jinshi Han, Siyuan Li, Wei Zhang, Mengjie Wei, Jingcheng Liu, Wei Wei, Xiaoya Liu, & Xiaojie Li. (2024). ACS Applied Polymer Materials(6). https://doi.org/10.1021/acsapm.3c02336
IEEE [1] Jinshi Han, Siyuan Li, Wei Zhang, Mengjie Wei, Jingcheng Liu, Wei Wei, Xiaoya Liu, and Xiaojie Li, ACS Applied Polymer Materials, no. 6, 2024, doi: 10.1021/acsapm.3c02336. keywords: {biosourced;azine;dynamic crosslinking networks;polyurethane elastomers;creep resistance;reprocessability}