High-Temperature Supercapacitors Based on MXene with Ultrahigh Volumetric Capacitance AITranslate

Changchun University of Technology; Changchun University of Technology; Changchun University of Technology; Changchun University of Technology; Changchun University of Technology; Changchun University of Technology; Changchun University of Technology; Changchun University of Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Currently, MXene-based supercapacitors (MSCs) have been widely studied due to their good flexibility and excellent electrochemical performance. At present, the application of supercapacitors is more and more extensive, which requires them to face various complex environments. However, MSCs applied under high-temperature conditions have not been reported. In this paper, the MXene–V2O5–polyaniline (MVP) ternary composite material is used as the electrode material, and sulfonated polybenzimidazole (SPBI) is used as the solid electrolyte to design high-temperature MSCs for the first time. The preparation of MVP is achieved by introducing V2O5 into the MXene layer and loading polyaniline (PANI) on its surface, which not only greatly improves the capacitance performance of the electrode but also ensures its stability at a high temperature. The capacitance value of the MVP electrode was as high as 3180 mF cm–3 (880 F g–1), with excellent mechanical properties and increased flexibility at the same time. Furthermore, the assembled supercapacitor has a high energy density of 79.2 Wh L–1 (22.1 Wh kg–1). Moreover, its capacitance value can reach 985.3 mF cm–3 (276 F g–1) at 120 °C. This work provides an efficient design of an energy storage device that can be used for high-temperature applications.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsmaterialslett.3c00223

Chinese Library Classification Number:

Citation Information:

Currently, MXene-based supercapacitors (MSCs) have been widely studied due to their good flexibility and excellent electrochemical performance. At present, the application of supercapacitors is more and more extensive, which requires them to face various complex environments. However, MSCs applied under high-temperature conditions have not been reported. In this paper, the MXene–V2O5–polyaniline (MVP) ternary composite material is used as the electrode material, and sulfonated polybenzimidazole (SPBI) is used as the solid electrolyte to design high-temperature MSCs for the first time. The preparation of MVP is achieved by introducing V2O5 into the MXene layer and loading polyaniline (PANI) on its surface, which not only greatly improves the capacitance performance of the electrode but also ensures its stability at a high temperature. The capacitance value of the MVP electrode was as high as 3180 mF cm–3 (880 F g–1), with excellent mechanical properties and increased flexibility at the same time. Furthermore, the assembled supercapacitor has a high energy density of 79.2 Wh L–1 (22.1 Wh kg–1). Moreover, its capacitance value can reach 985.3 mF cm–3 (276 F g–1) at 120 °C. This work provides an efficient design of an energy storage device that can be used for high-temperature applications.

quote

GB/T 7714-2015 [1] Chenglong Li, Shuang Wang, XiaoRui Wang, et al. ACS Materials Letters, 2023(5). DOI:10.1021/acsmaterialslett.3c00223.
MLA [1] Chenglong Li, et al., ACS Materials Letters, no. 5, 2023, https://doi.org/10.1021/acsmaterialslett.3c00223.
APA [1] Chenglong Li, Shuang Wang, XiaoRui Wang, Wenyu Bai, Han Sun, Feng Pan, Yue Chi, & Zhe Wang. (2023). ACS Materials Letters(5). https://doi.org/10.1021/acsmaterialslett.3c00223
IEEE [1] Chenglong Li, Shuang Wang, XiaoRui Wang, Wenyu Bai, Han Sun, Feng Pan, Yue Chi, and Zhe Wang, ACS Materials Letters, no. 5, 2023, doi: 10.1021/acsmaterialslett.3c00223.