Biodegradable Polymer Blends: Studies on Performance Control through Droplet to Co-continuous Morphology AITranslate

University of Guelph; University of Guelph; University of Guelph; University of Guelph; University of Guelph
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

This is the first-ever scientific report on melt blending of two tough home-compostable bioplastics, namely, bio-based poly(butylene succinate-co-adipate) (BioPBSA) and poly(butylene adipate-co-terephthalate) (PBAT). The micrographs from scanning electron microscopy showed that the morphology changed from a droplet-matrix to a co-continuous one as the PBAT concentration was increased in blends. Rheological studies revealed an increase in viscosity and storage modulus of some blends, specifically, the one with 30 wt % of PBAT, as compared to neat biopolymers, as evidence of compatibilization between two bioplastics. The crystallization temperature of PBAT reduced in the presence of BioPBSA, but the presence of a solid PBAT phase did not affect the crystallization of BioPBSA significantly. PBAT showed high capability to enhance the %elongation at break of BioPBSA except in blends with an equal concentration of biopolymers. The appropriate blends having balanced melt elasticity and %elongation show promise for flexible packaging uses as sustainable alternatives to their non-biodegradable plastics such as polyethylene.

KeyWords AITranslate

sustainable packaging biodegradable polymers singleuse plastics mechanical properties rheology morphology
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c00603

Chinese Library Classification Number:

Citation Information:

This is the first-ever scientific report on melt blending of two tough home-compostable bioplastics, namely, bio-based poly(butylene succinate-co-adipate) (BioPBSA) and poly(butylene adipate-co-terephthalate) (PBAT). The micrographs from scanning electron microscopy showed that the morphology changed from a droplet-matrix to a co-continuous one as the PBAT concentration was increased in blends. Rheological studies revealed an increase in viscosity and storage modulus of some blends, specifically, the one with 30 wt % of PBAT, as compared to neat biopolymers, as evidence of compatibilization between two bioplastics. The crystallization temperature of PBAT reduced in the presence of BioPBSA, but the presence of a solid PBAT phase did not affect the crystallization of BioPBSA significantly. PBAT showed high capability to enhance the %elongation at break of BioPBSA except in blends with an equal concentration of biopolymers. The appropriate blends having balanced melt elasticity and %elongation show promise for flexible packaging uses as sustainable alternatives to their non-biodegradable plastics such as polyethylene.

quote

GB/T 7714-2015 [1] Ehsan Pesaranhajiabbas, Akhilesh Kumar Pal, Arturo RodriguezUribe, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c00603.
MLA [1] Ehsan Pesaranhajiabbas, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c00603.
APA [1] Ehsan Pesaranhajiabbas, Akhilesh Kumar Pal, Arturo RodriguezUribe, Amar K. Mohanty, & Manjusri Misra. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c00603
IEEE [1] Ehsan Pesaranhajiabbas, Akhilesh Kumar Pal, Arturo RodriguezUribe, Amar K. Mohanty, and Manjusri Misra, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c00603. keywords: {sustainable packaging;biodegradable polymers;singleuse plastics;mechanical properties;rheology;morphology}